The Seebeck coefficients, electrical resistivities, total thermal conductivities, and magnetization are reported for temperatures between 5 and 350 K for n-type Bi0.88Sb0.12 nano-composite alloys made by Ho-doping at the 0, 1 and 3% atomic levels. The alloys were prepared using a dc hot-pressing method, and are shown to be single phase for both Ho contents with grain sizes on the average of 900 nm. We find the parent compound has a maximum of ZT = 0.28 at 231 K, while doping 1% Ho increases the maximum ZT to 0.31 at 221 K and the 3% doped sample suppresses the maximum ZT = 0.24 at a temperature of 260 K.

preprint2012arXivOpen access

Signal facts

What is known right now

Open access5 authors1 topic

Next steps

Decide what to do with this paper

Use like or dislike for the fast social read. The more specific scholarly feedback stays available below when needed.

Log in to curate

Reading frame

Keep the important context close to the paper

Keep the important signals around this paper in one place: votes, save state, collection context, reviews and the metadata you need before deciding what to do next.

Institutions

Add specific reaction

Move through the context

Research map

Open full explorer

Move through nearby people, institutions, topics and adjacent work without leaving the paper page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Structured reviews

0 review(s)

ContributeLeave structured feedbackUse the review template when you have a concrete strength, concern or method question.Open review form

No structured reviews yet. High-signal critique starts here.

Work discussion

0 comment(s)

DiscussAdd a high-signal commentKeep quick notes, caveats and replication pointers separate from formal reviews.Open comment form

No discussion yet. The first strong comment sets the tone.