Source author record

Jialei Tang

Jialei Tang appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.

ResearcherUnclaimed source record

Catalog footprint

What is connected

4works
1topics
4close collaborators

Actions

Connect this record

Log in to claim

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

4 published item(s)

preprint2014arXiv

Fabrication of an integrated high-quality-factor (high-Q) optofluidic sensor by femtosecond laser micromachining

We report on fabrication of a microtoroid resonator of a high-quality factor (i. e., Q-factor of ~3.24x10^6 measured under the critical coupling condition) integrated in a microfluidic channel using femtosecond laser three-dimensional (3D) micromachining. Coupling of light into and out of the microresonator has been realized with a fiber taper that is reliably assembled with the microtoroid. The assembly of the fiber to the microtoroid is achieved by welding the fiber taper onto the sidewall of the microtoroid using CO_2 laser irradiation. The integrated microresonator maintains a high Q-factor of 3.21x10^5 as measured in air, which should still be sufficient for many sensing applications. We test the functionality of the integrated optofluidic sensor by performing bulk refractive index sensing of purified water doped with tiny amount of salt. It is shown that a detection limit of ~1.2x10^-4 refractive index unit can be achieved. Our result showcases the capability of integration of high-Q microresonators with complex microfluidic systems using femtosecond laser 3D micromachining.

preprint2014arXiv

Fabrication of three-dimensional microdisk resonators in calcium fluoride by femtosecond laser micromachining

We report on fabrication of on-chip calcium fluoride (CaF2) microdisk resonators using water-assisted femtosecond laser micromachining. Focused ion beam (FIB) milling is used to create ultra-smooth sidewalls. The quality (Q)-factors of the fabricated microresonators are measured to be 4.2x10^4 at wavelengths near 1550 nm. The Q factor is mainly limited by the scattering from the bottom surface of the disk whose roughness remains high due to the femtosecond laser micromachining process. This technique facilitates formation of on-chip microresonators on various kinds of bulk crystalline materials, which can benefit a wide range of applications such as nonlinear optics, quantum optics, and chip-level integration of photonic devices.

preprint2014arXiv

Integration of an optical fiber taper with an optical microresonator fabricated in glass by femtosecond laser 3D micromachining

We report on fabrication of a microtoroid resonator of a high-quality factor (i. e., Q-factor of ~3.24x10^6 measured under the critical coupling condition) using femtosecond laser three-dimensional (3D) micromachining. Coupling of light into and out of the microresonator has been realized with a fiber taper that is reliably assembled with the microtoroid. The assembly of the fiber taper to the microtoroid is achieved by welding the fiber taper onto the sidewall of the microtoroid using CO2 laser irradiation. The integrated microresonator maintains a high Q-factor of 3.21x10^5 as measured in air.

preprint2014arXiv

On-chip tuning of the resonant wavelength in a high-Q microresonator integrated with a microheater

We report on fabrication of a microtoroid resonator of high-quality (high-Q) factor integrated with an on-chip microheater. Both the microresonator and microheater are fabricated using femtosecond laser three-dimensional (3D) micromachining. The microheater, which is located about 200 micron away from the microresonator, has a footprint size of 200 micron by 400 micron. Tuning of the resonant wavelength in the microresonator has been achieved by varying the voltage applied on the microheater. The drifting of the resonant wavelength shows a linear dependence on the square of the voltage applied on the microheater. We found that the response time of the microresonator is less than 10 secs which is significantly shorter than the time required for reaching a thermal equilibrium on conventional heating instruments such as an external electric heater.