Source author record

B. Samantaray

B. Samantaray appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.

ResearcherUnclaimed source record

Catalog footprint

What is connected

5works
4topics
4close collaborators

Actions

Connect this record

Log in to claim

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

5 published item(s)

preprint2021arXiv

Damping in yttrium iron garnet film with an interface

We report strong damping enhancement in a 200 nm thick yttrium iron garnet (YIG) film due to spin inhomogeneity at the interface. The growth-induced thin interfacial gadolinium iron garnet (GdIG) layer antiferromagnetically (AFM) exchange couples with the rest of the YIG layer. The out-of-plane angular variation of ferromagnetic resonance (FMR) linewidth $ΔH$ reflects a large inhomogeneous distribution of effective magnetization $Δ4 πM_{eff}$ due to the presence of an exchange springlike moments arrangement in YIG. We probe the spin inhomogeneity at the YIG-GdIG interface by performing an in-plane angular variation of resonance field $H_{r}$, leading to a unidirectional feature. The large extrinsic $Δ4πM_{eff}$ contribution, apart from the inherent intrinsic Gilbert contribution, manifests enhanced precessional damping in YIG film.

preprint2020arXiv

Ferromagnetic Resonance Studies of Strain tuned Bi:YIG Films

Bismuth-doped Yttrium iron garnet (Bi:YIG) thin films known for large Magneto-optical activity with low losses still needs to get probed for its magnetization dynamics. We demonstrate a controlled tuning of magnetocrystalline anisotropy in Bi-doped Y_3 Fe_5 O_12 (Bi:YIG) films of high crystalline quality using growth induced epitaxial strain on [111]-oriented Gd_3 Ga_5 O_12 (GGG) substrate. We optimize a growth protocol to get thick highly-strained epitaxial films showing large magneto-crystalline anisotropy, compare to thin films prepared using a different protocol. Ferromagnetic resonance measurements establish a linear dependence of the out-of-plane uniaxial anisotropy on the strain induced rhombohedral distortion of Bi:YIG lattice. Interestingly, the enhancement in the magnetoelastic constant due to an optimum substitution of Bi^(3+) ions with strong spin orbit coupling does not strongly affect the precessional damping (~2x10^(-3) ). Large magneto-optical activity, reasonably low damping, large magnetocrystalline anisotropy and large magnetoelastic coupling in BiYIG are the properties that may help BiYIG emerge as a possible material for photo-magnonics and other spintronics applications.

preprint2015arXiv

Giant magnetothermal conductivity and magnetostriction effect in charge ordered Nd$_{0.8}$Na$_{0.2}$MnO$_{3}$ compound

We present results on resistivity ($ρ$), magnetization ($M$), thermal conductivity ($κ$), magnetostriction ($\frac{ΔL}{L(0)}$) and specific heat ($C_{p}$) of charge-orbital ordered antiferromagnetic Nd$_{0.8}$Na$_{0.2}$MnO$_{3}$ compound. Magnetic field-induced antiferromagnetic/charge-orbital ordered insulating to ferromagnetic metallic transition leads to giant magnetothermal conductivity and magnetostriction effect. The low-temperature irreversibility behavior in $ρ$, $M$, $κ$ and $\frac{ΔL}{L(0)}$ due to field cycling together with striking similarity among the field and temperature dependence of these parameters manifest the presence of strong and complex spin-charge-lattice coupling in this compound. The giant magnetothermal conductivity is attributed mainly to the suppression of phonon scattering due to the destabilization of spin fluctuations and static/dynamic Jahn-Teller distortion by the application of magnetic field.

preprint2015arXiv

Perpendicular standing spin wave and magnetic anisotropic study on amorphous FeTaC films

Magnetic anisotropy, spin wave (SW) excitation and exchange stiffness constant of amorphous FeTaC ($d$ = 20-200 nm) films were studied as a function of thickness using micro-strip ferromagnetic resonance (MS-FMR) technique. The MS-FMR spectra for in-plane applied magnetic field show the presence of uniform precessional mode ($n$ = 0) along with first perpendicular standing spin wave (PSSW) mode ($n$ = 1) especially for $d$ = 50, 100 and 200 nm films. The angular ($φ_{H}$) dependence of resonance field ($H_{r}$) and magnetic field dependence of resonance frequencies ($f_{r}$) in planar configuration for the uniform and PSSW modes were modeled successfully by using dispersion relation which arises from a combination of exchange and dipolar interactions. The relevant parameters such as saturation magnetization ($4πM_{S}$), uniaxial anisotropic constant ($K_{u}$), $g$-factor, and exchange stiffness constants ($A_{ex}$) are estimated for different FeTaC film thickness. $A_{ex}$ is found to increase from 1.52(4)$\times$10$^{-7}$ to 5.0(5)$\times$10$^{-6}$ erg/cm as the thickness of film increases from 50 to 200 nm, possibly due to surface pinning effect or significant inhomogeneity especially at higher thickness films.

preprint2015arXiv

Spin dynamics and frequency dependence of magnetic damping study in soft ferromagnetic FeTaC film with a stripe domain structure

Perpendicular magnetic anisotropy (PMA) and low magnetic damping are the key factors for the free layer magnetization switching by spin transfer torque technique in magnetic tunnel junction devices. The magnetization precessional dynamics in soft ferromagnetic FeTaC thin film with a stripe domain structure was explored in broad band frequency range by employing micro-strip ferromagnetic resonance technique. The polar angular variation of resonance field and linewidth at different frequencies have been analyzed numerically using Landau-Lifshitz-Gilbert equation by taking into account the total free energy density of the film. The numerically estimated parameters Landé $g$-factor, PMA constant, and effective magnetization are found to be 2.1, 2$\times10^{5}$ erg/cm$^{3}$ and 7145 Oe, respectively. The frequency dependence of Gilbert damping parameter ($α$) is evaluated by considering both intrinsic and extrinsic effects into the total linewidth analysis. The value of $α$ is found to be 0.006 at 10 GHz and it increases with decreasing precessional frequency.