Abstract
Nano/micro-scale mechanical properties of multiferroic materials can be controlled by the external magnetic or electric field due to the coupling interaction. For the first time, a modularized multi-field nanoindentation apparatus for carrying out testing on materials in external magnetostatic/electrostatic field is constructed. Technical issues, such as the application of magnetic/electric field and the processes to diminish the interference between external fields and the other parts of the apparatus, are addressed. Tests on calibration specimen indicate the feasibility of the apparatus. The load-displacement curves of ferromagnetic, ferroelectric and magnetoelectric materials in the presence/absence of external fields reveal the small-scale magnetomechanical and electromechanical coupling, showing as the Delta-E and Delta-H effects, i.e. the magnetic/electric field induced changes in the apparent elastic modulus and indentation hardness.
Connections
Explore this paper’s authors, topics and related work.
Building this map preview
BZPEER is loading the nearby papers, people, topics and institutions for this page.
Reviews 0
Write a review
No reviews yet.
Discussion 0
Add a comment
No comments yet.