Abstract
PbZr0.52Ti0.48O3/La0.67Sr0.33MnO3(PZT/LSMO) bilayer with surface roughness ~ 1.8 nm thin films have been grown by pulsed laser deposition on LaAlO3(LAO) substrates. High remnant polarization (30-54 micro C/cm2), dielectric constant(400-1700), and well saturated magnetization were observed depending upon the deposition temperature of the ferromagnetic layer and applied frequencies. Giant frequency-dependent change in dielectric constant and loss were observed above the ferromagnetic-paramagnetic temperature. The frequency dependent dielectric anomalies are attributed to the change in metallic and magnetic nature of LSMO and also the interfacial effect across the bilayer; an enhanced magnetoelectric interaction may be due to the Parish-Littlewood mechanism of inhomogeneity near the metal-dielectric interface.
Connections
Explore this paper’s authors, topics and related work.
Building this map preview
BZPEER is loading the nearby papers, people, topics and institutions for this page.
Reviews 0
Write a review
No reviews yet.
Discussion 0
Add a comment
No comments yet.