Abstract

High quality single crystals of WTe2_2 were grown using a Te flux followed by a cleaning step involving self-vapor transport. The method is reproducible and yields consistently higher quality single crystals than are typically obtained via halide assisted vapor transport methods. Magnetoresistance (MR)values at 9 Tesla and 2 Kelvin as high as 1.75 million \%, nearly an order of magnitude higher than previously reported for this material, were obtained on crystals with residual resistivity ratio (RRR) of approximately 1250. The MR follows a near B2^2 law (B = 1.95(1)) and, assuming a semiclassical model, the average carrier mobility for the highest quality crystal was found to be ~167,000 cm2^2/Vs at 2 K. A correlation of RRR, MR ratio and average carrier mobility (μavgμ_{avg}) is found with the cooling rate during the flux growth.

Explore this paper’s authors, topics and related work.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Reviews 0

Write a reviewWrite

No reviews yet.

Discussion 0

Add a commentWrite

No comments yet.