preprint2014arXiv

Suppression of superconductivity and structural phase transition against pressure in Ca10_{10}(Ir4_{4}As8_{8})(Fe2−x_{2-x}Irx_{x}As2_{2})5_{5}

We measured the pressure dependence of in-plane resistivity ρabρ_{ab} in the recently-discovered iron-based superconductor Ca10_{10}(Ir4_{4}As8_{8})(Fe2−x_{2-x}Irx_{x}As2_{2})5_{5}, which shows a unique structural phase transition in the absence of magnetic ordering, with a superconducting transition temperature TcT_{\rm c} = 16 K and structural phase transition temperature TsT_{\rm s} ≃\simeq 100 K at ambient pressure. TcT_{\rm c} and TsT_{\rm s} are suppressed on applying pressure and disappear at approximately 0.5 GPa, suggesting a relationship between superconductivity and structure. Ca10_{10}(Ir4_{4}As8_{8})(Fe2−x_{2-x}Irx_{x}As2_{2})5_{5} is a rather rare example in which the superconductivity appears only in a low-temperature ordered phase. The fact that the change in the crystal structure is directly linked with superconductivity suggests that the crystal structure as well as magnetism are important factors governing superconductivity in iron pnictides.

preprint2013arXiv

Pressure-Induced Superconductivity in Mineral Calaverite AuTe2

The pressure dependences of resistivity and ac susceptibility have been measured in the mineral calaverite AuTe2_2. Resistivity clearly shows a first-order phase transition into a high-pressure phase, consistent with the results of a previous structural analysis. We found zero resistivity and a diamagnetic shielding signal at low temperatures in the high-pressure phase, which clearly indicates the appearance of superconductivity. Our experimental results suggest that bulk superconductivity appears only in the high-pressure phase. For AuTe2_2, the highest superconducting transition temperature under pressure is TcT_{\rm c} = 2.3 K at 2.34 GPa; it was TcT_{\rm c} = 4.0 K for Pt-doped (Au0.65_{0.65}Pt0.35_{0.35})Te2_2. The difference in TcT_{\rm c} between the two systems is discussed on the basis of the results obtained using the band calculations and McMillan's formula.

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.