Source author record

Hideki Kajitani

Hideki Kajitani appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.

ResearcherUnclaimed source record

Catalog footprint

What is connected

2works
1topics
4close collaborators

Actions

Connect this record

Log in to claim

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

2 published item(s)

preprint2016arXiv

Enhancement of critical current densities in (Ba,K)Fe2As2 wires and tapes using HIP technique

(Ba,K)Fe2As2 superconducting wires and tapes are fabricated by using hot isostatic pressing (HIP) technique, and their superconducting properties are studied. In the HIP round wire, transport critical current density (Jc) at 4.2 K has achieved record-high value of 175 kA/cm2 at zero field, and exceeds 20 kA/cm2 even at 100 kOe. Improvement of polycrystalline powder synthesis may play a key role for the enhancement of Jc. In the HIP tape, even larger transport Jc of 380 kA/cm2 is realized at zero field. Based on magnetization and magneto-optical measurements, possible further enhancement of Jc is discussed.

preprint2013arXiv

Enhancement of Critical Current Densities in (Ba,K)Fe2As2 by 320 MeV Au Irradiation in Single Crystals and by High-Pressure Sintering in PIT Wires

We demonstrate a large enhancement of critical current density (Jc) up to 1.0x10^7 A/cm2 at 5 K under self-field in (Ba,K)Fe2As2 single crystals by irradiating 320 MeV Au ions. With the very promising potential of this material in mind, we have fabricated a (Ba,K)Fe2As2 superconducting wire through a powder-in-tube method combined with the hot isostatic pressing technique, whose effectiveness has been proven in industrial Bi2223 tapes. The Jc in the wire at 4.2 K has reached 37 kA/cm2 under self-field and 3.0 kA/cm2 at 90 kOe. Magneto-optical imaging of the wire confirmed the large intergranular Jc in the wire core.