Large Negative Electronic Compressibility of LaAlO3-SrTiO3 Interfaces with Ultrathin LaAlO3 Layers

preprint2012arXivOpen access

Abstract

A two-dimensional electron liquid is formed at the n-type interface between SrTiO3 and LaAlO3. Here we report on Kelvin probe microscopy measurements of the electronic compressibility of this electron system. The electronic compressibility is found to be negative for carrier densities of \approx10^13/cm^2. At even smaller densities, a metal-to-insulator transition occurs. These local measurements corroborate earlier measurements of the electronic compressibility of LaAlO3-SrTiO3 interfaces obtained by measuring the capacitance of macroscopic metal-LaAlO3-SrTiO3 capacitors.