Electronic charges and electric potential at LaAlO3/SrTiO3 interfaces studied by core-level photoemission spectroscopy

We studied LaAlO3/SrTiO3 interfaces for varying LaAlO3 thickness by core-level photoemission spectroscopy. In Ti 2p spectra for conducting "n-type" interfaces, Ti3+ signals appeared, which were absent for insulating "p-type" interfaces. The Ti3+ signals increased with LaAlO3 thickness, but started well below the critical thickness of 4 unit cells for metallic transport. Core-level shifts with LaAlO3 thickness were much smaller than predicted by the polar catastrophe model. We attribute these observations to surface defects/adsorbates providing charges to the interface even below the critical thickness.

preprint2011arXivOpen access
0citations
0reviews
0saves
Nocode
Nodataset
0institutions

Next steps

Decide what to do with this paper

Use like or dislike for the fast social read. The more specific scholarly feedback stays available below when needed.

Log in to curate

Reading frame

Keep the important context close to the paper

Keep the important signals around this paper in one place: votes, save state, collection context, reviews and the metadata you need before deciding what to do next.

Institutions

Add specific reaction

Move through the context

Research map

Open full explorer

Move through nearby people, institutions, topics and adjacent work without leaving the paper page.

Building this graph slice

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Structured reviews

0 review(s)

ContributeLeave structured feedbackUse the review template when you have a concrete strength, concern or method question.Open review form

No structured reviews yet. High-signal critique starts here.

Work discussion

0 comment(s)

DiscussAdd a high-signal commentKeep quick notes, caveats and replication pointers separate from formal reviews.Open comment form

No discussion yet. The first strong comment sets the tone.