A Comparison of Stripe Modulations in La1.875_{1.875}Ba0.125_{0.125}CuO4_4 and La1.48_{1.48}Nd0.4_{0.4}Sr0.12_{0.12}CuO4_4

preprint2011arXivOpen access

Abstract

We report combined soft and hard x-ray scattering studies of the electronic and lattice modulations associated with stripe order in La1.875_{1.875}Ba0.125_{0.125}CuO4_4 and La1.48_{1.48}Nd0.4_{0.4}Sr0.12_{0.12}CuO4_4. We find that the amplitude of both the electronic modulation of the hole density and the strain modulation of the lattice is significantly larger in La1.875_{1.875}Ba0.125_{0.125}CuO4_4 than in La1.48_{1.48}Nd0.4_{0.4}Sr0.12_{0.12}CuO4_4 and is also better correlated. The in-plane correlation lengths are isotropic in each case; for La1.875_{1.875}Ba0.125_{0.125}CuO4_4, ξhole=255±5ξ^{hole}=255\pm 5 Å whereas for La1.48_{1.48}Nd0.4_{0.4}Sr0.12_{0.12}CuO4_4F, ξhole=111±7ξ^{hole}=111\pm 7 Å. We find that the modulations are temperature independent in La1.875_{1.875}Ba0.125_{0.125}CuO4_4 in the low temperature tetragonal phase. In contrast, in La1.48_{1.48}Nd0.4_{0.4}Sr0.12_{0.12}CuO4_4, the amplitude grows smoothly from zero, beginning 13 K below the LTT phase transition. We speculate that the reduced average tilt angle in La1.875_{1.875}Ba0.125_{0.125}CuO4_4 results in reduced charge localization and incoherent pinning, leading to the longer correlation length and enhanced periodic modulation amplitude.

Explore this paper’s authors, topics and related work.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Reviews 0

Write a reviewWrite

No reviews yet.

Discussion 0

Add a commentWrite

No comments yet.