Researcher profile

Vladimir Khovaylo

Vladimir Khovaylo contributes to research discovery and scholarly infrastructure.

ResearcherAffiliation not importedOpen to collaborate

Trust snapshot

Quick read

Trust 21 - EmergingVerification L1Unclaimed author
6works
0followers
5topics
4close collaborators

Actions

Decide how to stay connected

Follow researcher0

Identity and collaboration

How to connect with this researcher

Claiming links this public author record to a researcher profile and unlocks direct collaboration workflows.

Log in to claim

Direct collaboration

Open a focused conversation when the fit is right

Claim this author entity first to unlock direct invitations.

Research graph

See the researcher in context

Open full explorer

Inspect adjacent work, topics, institutions and collaborators without jumping out to a separate graph page.

Building this graph slice

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

6 published item(s)

preprint2022arXiv

A study on rare-earth Laves phases for magnetocaloric liquefaction of hydrogen

We are witnessing a great transition towards a society powered by renewable energies to meet the ever-stringent climate target. Hydrogen, as an energy carrier, will play a key role in building a climate-neutral society. Although liquid hydrogen is essential for hydrogen storage and transportation, liquefying hydrogen is costly with the conventional methods based on Joule-Thomas effect. As an emerging technology which is potentially more efficient, magnetocaloric hydrogen liquefaction is a "game-changer". In this work, we have investigated the rare-earth-based Laves phases ${\rm R}Al_2$ and ${\rm R}Ni_2$ for magnetocaloric hydrogen liquefaction. We have noticed an unaddressed feature that the magnetocaloric effect of second-order magnetocaloric materials can become "giant" near the hydrogen boiling point. This feature indicates strong correlations, down to the boiling point of hydrogen, among the three important quantities of the magnetocaloric effect: the maximum magnetic entropy change $ΔS_{m}^{max}$, the maximum adiabatic temperature change $ΔT_{ad}^{max}$, and the Curie temperature $T_C$. Via a comprehensive literature review, we interpret the correlations for a rare-earth intermetallic series as two trends: (1) $ΔS_{m}^{max}$ increases with decreasing $T_C$; (2) $ΔT_{ad}^{max}$ decreases near room temperature with decreasing $T_C$ but increases at cryogenic temperatures. Moreover, we have developed a mean-field approach to describe these two trends theoretically. The dependence of $ΔS_{m}^{max}$ and $ΔT_{ad}^{max}$ on $T_C$ revealed in this work helps us quickly anticipate the magnetocaloric performance of rare-earth-based compounds, guiding material design and accelerating the discoveries of magnetocaloric materials for hydrogen liquefaction.

preprint2022arXiv

Influence of Bi substitution with rare-earth elements on the transport properties of BiCuSeO oxyselenides

In this study, we demonstrate that introducing of rare-earth elements, $R$ = La or Pr, into the Bi-O charge reservoir layer of BiCuSeO leads to an increase of both, the charge carrier concentration and the effective mass. Although the charge carrier mobility slightly decreases upon Bi$^{3+}$ to $R^{3+}$ substitution, the electronic transport properties are significantly improved in a broad temperature range from 100 K to 800 K. In particular, the electrical resistivity decreases by two times, while the Seebeck coefficient drops from 323 $μ$V K$^{-1}$ to 238 $μ$V K$^{-1}$ at 800 K. Thus, a power factor of nearly 3 $μ$W cm$^{-1}$ K$^{-2}$ is achieved for Bi$_{0.92}$La$_{0.08}$CuSeO sample at 800 K. Meanwhile, a noticeable decrease of the lattice thermal conductivity is observed for the substituted samples, which can be attributed to the enhanced point defect scattering mostly originated from atomic mass fluctuations between $R$ and Bi. Ultimately, a maximum $zT$ value of nearly 0.34 at 800 K is obtained for the Bi$_{0.92}$La$_{0.08}$CuSeO sample, which is ~30% higher than that of pristine BiCuSeO.

preprint2022arXiv

Substantial enhancement in thermoelectric figure-of-merit of half Heusler ZrNiPb alloys

Ternary half Heusler alloys are under intense investigations recently towards achieving high thermoelectric figure-of-merit (ZT). Of particular interest is the ZrNiPb based half Heusler (HH) alloy where an optimal value of ZT = 0.7 at 773 K has been achieved by co-doping Sn and Bi at Pb site. In this work, we identify an excellent ZT of 1.3 in ZrNi1+xPb0.38Sn0.6Bi0.02 (x= 0.03, at 773 K) composite alloy. This is achieved by synergistic modulation of electronic as well as thermal properties via introduction of minor phase of full Heusler (FH) in the HH matrix through compositional tuning approach. These Ni-rich ZrNi1+xPb0.38Sn0.6Bi0.02 alloys were synthesized via Arc melting followed by consolidation via Spark Plasma Sintering (SPS). These alloys were characterized by XRD and SEM that shows formation of nanocomposites comprising of HH matrix phase and FH secondary minor phases. Enhancement in ZT is mainly attributed to a synchronized increase in power factor and about 25% decrease in its thermal conductivity. The thermoelectric compatibility factor (S) is also calculated for all samples. The theoretically calculated thermoelectric device efficiency of best performing sample ZrNi1.03Pb0.38Sn0.6Bi0.02 is estimated to be 13.6%. Our results imply that controlled fine tuning in HH compounds through compositional tuning approach would lead to novel off-stoichiometric HH phases with enhanced ZT value for efficient thermoelectric device fabrication.

preprint2022arXiv

Thermoelectric properties of Sm-doped BiCuSeO oxyselenides fabricated by two-step reactive sintering

Among layered oxygen-containing compounds, BiCuSeO is one of the most promising candidates for thermoelectric applications due to its intrinsically low thermal conductivity and good thermal stability. However, the rather poor electrical conductivity of pristine BiCuSeO hinders its potential. Further enhancement of the thermoelectric performance by single doping at Bi site is limited mainly due to dramatic decrease of carrier mobility. Thus, new strategies, such as dual doping or doping with variable-valence elements seem to be promising. Along with that, the development of a fast and scalable synthesis route is essential for the industrial-scale fabrication of thermoelectric materials. Hence, in this paper, Bi$_{1-x}$Sm$_{x}$CuSeO samples (0 $\leq$ $x$ $\leq$ 0.08) have been synthesized with a simple and scalable reactive sintering process. For comparison, Bi$_{1-x}$Sm$_{x}$CuSeO oxyselenides were also obtained by the conventional solid-state route. Our results highlight that, Sm for Bi substitution increases the electrical conductivity by 1.5 - 2 times and decreases the Seebeck coefficient by ~1.4 times at 873 K for both series. Overall, considering the increase of lattice thermal conductivity upon doping and not optimized power factor, the figure of merit $zT$ is reducing upon doping.

preprint2020arXiv

Direct synthesis of p-type bulk BiCuSeO oxyselenides by reactive spark plasma sintering and related thermoelectric properties

Herein, we demonstrate that BiCuSeO compound can be formed in bulk directly from the raw materials through reactive spark plasma sintering (RSPS) followed by ball milling and a second short spark plasma sintering step. Compared to BiCuSeO samples obtained by a conventional solid-state reaction, the electrical transport properties of the RSPS bulk were moderately affected by the sintering technique, while the lattice thermal conductivity was almost unaffected, and the figure of merit zT attained a value at 773 K comparable to state-of-the-art BiCuSeO. The results indicate a new scalable method for the preparation of oxyselenides.

preprint2019arXiv

Ultrafast synthesis of Pb-doped BiCuSeO oxyselenides by high-energy ball milling

We report on the direct ultrafast synthesis of Pb-doped BiCuSeO oxyselenides by high-energy ball milling. We show that, contrary to the mechanical alloying sintering routes used in the previous reports which require 7 - 13 hours to fabricate the BiCuSeO phase in powder form, this synthesis technique enables us to obtain pure phase materials at room temperature under air with milling time less than 60 minutes.