Source author record

D. W. Hewak

D. W. Hewak appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.

ResearcherUnclaimed source record

Catalog footprint

What is connected

3works
2topics
4close collaborators

Actions

Connect this record

Log in to claim

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

3 published item(s)

preprint2020arXiv

Intense Anti-Stokes Emission of Erbium Ions in Gallium Lanthanum Sulphide-Oxide Glass in Visible Spectral Range

Photoluminescence spectra have been investigated in erbium doped GaLaS(O) glasses. The samples demonstrate intense green emission bands centered at around 525 and 550 nm due to up-conversion processes in erbium ions. The theoretical description of up-conversion intensity as a function of excitation intensity has been offered. It is based on a solution of a system of rate equations taking into account three up-conversion transitions.

preprint2014arXiv

Concentration dependence of the fluorescence decay profile in transition metal doped chalcogenide glass

In this paper we present the fluorescence decay profiles of vanadium and titanium doped gallium lanthanum sulphide (GLS) glass at various doping concentrations between 0.01 and 1% (molar). We demonstrate that below a critical doping concentration the fluorescence decay profile can be fitted with the stretched exponential function: exp[-(t/τ)\b{eta}], where τ is the fluorescence lifetime and \b{eta} is the stretch factor. At low concentrations the lifetime for vanadium and titanium doped GLS was 30 μs and 67 μs respectively. We validate the use of the stretched exponential model and discuss the possible microscopic phenomenon it arises from. We also demonstrate that above a critical doping concentration of around 0.1% (molar) the fluorescence decay profile can be fitted with the double exponential function: a*exp-(t/τ1)+ b*exp-(t/τ2), where τ1and τ2 are characteristic fast and slow components of the fluorescence decay profile, for vanadium the fast and slow components are 5 μs and 30 μs respectively and for titanium they are 15 μs and 67 μs respectively. We also show that the fluorescence lifetime of vanadium and titanium at low concentrations in the oxide rich host gallium lanthanum oxy-sulphide (GLSO) is 43 μs and 97 μs respectively, which is longer than that in GLS. From this we deduce that vanadium and titanium fluorescing ions preferentially substitute into high efficiency oxide sites until at a critical concentration they become saturated and low efficiency sulphide sites start to be filled.

preprint2009arXiv

Phase-change chalcogenide glass metamaterial

Combining metamaterials with functional media brings a new dimension to their performance. Here we demonstrate substantial resonance frequency tuning in a photonic metamaterial hybridized with an electrically/optically switchable chalcogenide glass. The transition between amorphous and crystalline forms brings about a 10% shift in the near-infrared resonance wavelength of an asymmetric split-ring array, providing transmission modulation functionality with a contrast ratio of 4:1 in a device of sub-wavelength thickness.