Source author record

C. Tuisan

C. Tuisan appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.

ResearcherUnclaimed source record

Catalog footprint

What is connected

3works
1topics
4close collaborators

Actions

Connect this record

Log in to claim

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

3 published item(s)

preprint2015arXiv

Effective 90-degree magnetization rotation in Co2FeAl thin film/Piezoelectric system probed by microstripline ferromagnetic

Microstripline ferromagnetic resonance technique has been used to study the indirect magnetoelectric coupling occurring in an artificial magnetoelectric heterostructure consisting of a magnetostrictive thin film cemented onto a piezoelectric actuator. Two different modes (sweep-field and sweep-frequency modes) of this technique have been employed to quantitatively probe the indirect magnetoelectric coupling and to observe a voltage induced magnetization rotation (of 90 degree). This latter has been validated by the experimental frequency variation of the uniform mode and by the amplitude of the sweep-frequency spectra.

preprint2014arXiv

Co2FeAl Heusler thin films grown on Si and MgO substrates: annealing temperature effect

10 nm and 50 nm Co$_{2}$FeAl (CFA) thin films have been deposited on MgO(001) and Si(001) substrates by magnetron sputtering and annealed at different temperatures. X-rays diffraction revealed polycrystalline or epitaxial growth (according to the relation CFA(001)[110]//MgO(001)[100] epitaxial relation), respectively for CFA films grown on a Si and on a MgO substrate. For these later, the chemical order varies from the A2 phase to the B2 phase when increasing the annealing temperature (Ta) while only the A2 disorder type has been observed for CFA grown on Si. Microstrip ferromagnetic resonance (MS-FMR) measurements revealed that the in-plane anisotropy results from the superposition of a uniaxial and of a fourfold symmetry term for CFA grown on MgO substrates. This fourfold anisotropy, which disappears completely for samples grown on Si, is in accord with the crystal structure of the samples. The fourfold anisotropy field decreases when increasing Ta while the uniaxial anisotropy field is nearly unaffected by Ta within the investigated range. The MS-FMR data also allow for concluding that the gyromagnetic factor remains constant and that the exchange stiffness constant increases with $T_{a}$. Finally, the FMR linewidth decreases when increasing Ta, due to the enhancement of the chemical order. We derive a very low intrinsic damping parameter (1.3*10^-3 and 1.1*10^-3 for films of 50 nm thickness annealed at 615 °C grown on MgO and on Si, respectively).

preprint2014arXiv

Magnetic and structural properties of Co2FeAl thin films grown on Si substrate

The correlation between magnetic and structural properties of Co_{2} FeAl (CFA) thin films of different thickness (10 nm<d< 100 nm) grown at room temperature on MgO-buffered Si/SiO2 substrates and annealed at 600\lyxmathsym{\textdegree}C has been studied. XRD measurements revealed an (011) out-of-plane texture growth of the films. The deduced lattice parameter increases with the film thickness. Moreover, pole figures showed no in-plane preferential growth orientation. The magneto-optical Kerr effect hysteresis loops showed the presence of a weak in-plane uniaxial anisotropy with a random easy axis direction. The coercive field measured with an applied field along the easy axis direction and the uniaxial anisotropy field increase linearly with the inverse of the CFA thickness. The microstrip line ferromagnetic resonance measurements for in-plane and perpendicular applied magnetic fields revealed that the effective magnetization and the uniaxial in-palne anisotropy field follow a linear variation versus the inverse CFA thickness. This allows deriving a perpendicular surface anisotropy coefficient of -1.86 erg/cm2