Researcher profile

Binhan Sun

Binhan Sun contributes to research discovery and scholarly infrastructure.

ResearcherAffiliation not importedOpen to collaborate

Trust snapshot

Quick read

Trust 15 - UnverifiedVerification L1Unclaimed author
3works
0followers
1topics
4close collaborators

Actions

Decide how to stay connected

Follow researcher0

Identity and collaboration

How to connect with this researcher

Claiming links this public author record to a researcher profile and unlocks direct collaboration workflows.

Log in to claim

Direct collaboration

Open a focused conversation when the fit is right

Claim this author entity first to unlock direct invitations.

Research graph

See the researcher in context

Open full explorer

Inspect adjacent work, topics, institutions and collaborators without jumping out to a separate graph page.

Building this graph slice

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

3 published item(s)

preprint2022arXiv

Hydrogen trapping and embrittlement in high-strength Al-alloys

Ever more stringent regulations on greenhouse gas emissions from transportation motivate efforts to revisit materials used for vehicles. High-strength Al-alloys often used in aircrafts could help reduce the weight of automobiles, but are susceptible to environmental degradation. Hydrogen (H) "embrittlement" is often pointed as the main culprit, however, the mechanisms underpinning failure are elusive: atomic-scale analysis of H inside an alloy remains a challenge, and this prevents deploying alloy design strategies to enhance the materials' durability. Here we successfully performed near-atomic scale analysis of H trapped in second-phase particles and at grain boundaries in a high-strength 7xxx Al-alloy. We used these observations to guide atomistic ab-initio calculations which show that the co-segregation of alloying elements and H favours grain boundary decohesion, while the strong partitioning of H into the second-phases removes solute H from the matrix, hence preventing H-embrittlement. Our insights further advance the mechanistic understanding of H-assisted embrittlement in Al-alloys, emphasizing the role of H-traps in retarding cracking and guiding new alloy design.

preprint2020arXiv

Comparative study of hydrogen embrittlement resistance between additively and conventionally manufactured austenitic stainless steels

Hydrogen embrittlement in 304L (18wt.% Cr, 8-10wt.% Ni) austenitic stainless steel (ASS) fabricated by laser powder-bed-fusion (LPBF) was investigated by tensile testing after electrochemical hydrogen pre-charging and compared to conventionally available 304L ASSs with two different processing histories, (i) casting plus annealing (CA) and (ii) CA plus thermomechanical treatment (TMT). It was revealed that hydrogen-charging led to a significant reduction in ductility for the CA sample, but only a small effect of hydrogen was observed for the LPBF and CA-TMT samples. Hydrogen-assisted cracking behavior was found to be strongly linked to strain-induced martensitic transformation. In addition, the amount of alpha' martensite was much higher in the CA sample than in other samples, suggesting that severe hydrogen embrittlement can be correlated with the low mechanical stability of austenite. Detailed microstructural characterization showed that low austenite stability of the CA sample was mainly attributed to the retained content of delta ferrite and the chemical inhomogeneity inside the gamma matrix (gamma close to delta has ~2 wt.% higher Cr but ~2 wt.% lower Ni), but TMT enhanced the chemical homogeneity and thus austenite stability. By contrast, the LPBF process led directly, i.e. without any thermomechanical treatment, to a fully austenitic structure with homogeneous elemental distribution in the ASS. These results confirmed that the presence of delta and the chemical inhomogeneity inside gamma matrix, which promoted the deformation-induced martensitic transformation and the associated H enrichment at the gamma-alpha' interface, was the primary reason for the severe H-assisted failure.

preprint2020arXiv

Solute hydrogen and deuterium observed at the near atomic scale in high-strength steel

Observing solute hydrogen (H) in matter is a formidable challenge, yet, enabling quantitative imaging of H at the atomic-scale is critical to understand its deleterious influence on the mechanical strength of many metallic alloys that has resulted in many catastrophic failures of engineering parts and structures. Here, we report on the APT analysis of hydrogen (H) and deuterium (D) within the nanostructure of an ultra-high strength steel with high resistance to hydrogen embrittlement. Cold drawn, severely deformed pearlitic steel wires (Fe-0.98C-0.31Mn-0.20Si-0.20Cr-0.01Cu-0.006P-0.007S wt.%, ε=3.1) contains cementite decomposed during the pre-deformation of the alloy and ferrite. We find H and D within the decomposed cementite, and at some interfaces with the surrounding ferrite. To ascertain the origin of the H/D signal obtained in APT, we explored a series of experimental workflows including cryogenic specimen preparation and cryogenic-vacuum transfer from the preparation into a state-of-the-art atom probe. Our study points to the critical role of the preparation, i.e. the possible saturation of H-trapping sites during electrochemical polishing, how these can be alleviated by the use of an outgassing treatment, cryogenic preparation and transfer prior to charging. Accommodation of large amounts of H in the under-stoichiometric carbide likely explains the resistance of pearlite against hydrogen embrittlement.