Abstract
Recently, the magnetic moment/Mn, , in MnSi was measured to be 5.0 /Mn, at =0.1%. To understand this observed , we investigate several MnSi models of alloys using first-principles density functional methods. The only model giving was a 513-atom cell having the Mn at a substitutional site, and Si at a second-neighbor interstitial site. The observed large moment is a consequence of the weakened d-p hybridization between the Mn and one of its nearest neighbor Si atoms, resulting from the introduction of the second-neighbor interstitial Si. Our result suggests a way to tune the magnetic moments of transition metal doped semiconductors.