Abstract

Atomic layer deposition allows for precise control over film thickness and conformality. It is a critical enabler of high aspect ratio structures, such as 3D NAND memory, since its self-limiting behavior enables higher conformality than conventional processes. However, as the aspect ratio increases, deviations from complete conformality frequently occur, requiring comprehensive modeling to aid the development of novel technologies. To that end, we present a model for surface coverage during atomic layer deposition where incomplete conformality is present. This model combines existing approaches based on Knudsen diffusion and Langmuir kinetics. Our model expands the state-of-the art by (i) incorporating gas-phase diffusivity through the Bosanquet formula as well as reaction reversibility in the modeling framework first proposed by Yanguas-Gil and Elam, and (ii) being efficiently integrated within level-set topography simulators. The model is manually calibrated to published results of the prototypical atomic layer deposition of Al2_2O3_3 from TMA and H2_2O in lateral high aspect ratio structures. We investigate the temperature dependence of the H2_2O step, thus extracting an activation energy of 0.178 eV0.178\,\mathrm{eV} which is consistent with recent experiments. In the TMA step, we observe increased accuracy from the Bosanquet formula and we reproduce multiple independent experiments with the same parameter set, highlighting that the model parameters effectively capture the reactor conditions.

Explore this paper’s authors, topics and related work.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Reviews 0

Write a reviewWrite

No reviews yet.

Discussion 0

Add a commentWrite

No comments yet.