Abstract
The paper reports on the preparation of xenotime-structured ceramics by the Spark Plasma Sintering (SPS) method. Phosphates YGdPO (YPO:Gd) were obtained by the sol-gel method. The synthesized nanopowders are collected in large agglomerates 10-50 mkm in size. Ceramics has a fine-grained microstructure and a high relative density (98.67%). The total time of the SPS process was approximately 18 min. High-density sintered ceramics YPO:Gd with a xenotime structure were irradiated with Xe ions (E = 167 MeV) to fluences of - cm. Complete amorphization at maximum fluence was not achieved. As the fluence increases, an insignificant increase in the depth of the amorphous layer is observed. According to the results of grazing incidence XRD (GIXRD), with an increase in fluence from - cm, an increase in the volume fraction of the amorphous structure from 20 to 70% is observed. The intensity of XRD peak 200 YPO:Gd after recovery annealing (700C, 18 h) reached a value of ~80% of the initial intensity I0.
Connections
Explore this paper’s authors, topics and related work.
Building this map preview
BZPEER is loading the nearby papers, people, topics and institutions for this page.
Reviews 0
Write a review
No reviews yet.
Discussion 0
Add a comment
No comments yet.