Abstract
Here we report a record thermoelectric power factor of up to 160 W m-1 K-2 for the conjugated polymer poly(3-hexylthiophene) (P3HT). This result is achieved through the combination of high-temperature rubbing of thin films together with the use of a large molybdenum dithiolene p-dopant with a high electron affinity. Comparison of the UV-vis-NIR spectra of the chemically doped samples to electrochemically oxidized material reveals an oxidation level of 10%, i.e. one polaron for every 10 repeat units. The high power factor arises due to an increase in the charge-carrier mobility and hence electrical conductivity along the rubbing direction. We conclude that P3HT, with its facile synthesis and outstanding processability, should not be ruled out as a potential thermoelectric material.
Connections
Explore this paper’s authors, topics and related work.
Building this map preview
BZPEER is loading the nearby papers, people, topics and institutions for this page.
Reviews 0
Write a review
No reviews yet.
Discussion 0
Add a comment
No comments yet.