Emergence of Spin Ice freezing in Dy2_2Ti1.8_{1.8}Mn0.2_{0.2}O7_7

preprint2022arXivOpen access

Abstract

We herein present the spin freezing dynamics of stuffed polycrystalline compound Dy2_2Ti1.8_{1.8}Mn0.2_{0.2}O7_7. In Dy2_2Ti2_2O7_7, spin freezes with ice-like spin relaxations at a temperature around 3 K (Ti_i) along with another spin freezing at a temperature around 0.7 K (T\textless Ti_i). These relaxations can be observed prominently with an application of varying DC magnetic field bias and applied AC-field. We show here that with fractional inclusion of Mn at the Ti site in Dy2_2Ti2_2O7_7, there is a significant shift in these temperatures. In Dy2_2Ti1.8_{1.8}Mn0.2_{0.2}O7_7 the Ti_i shifts to a higher temperature around 5 K and freezing belonging to T\textless Ti_i shifts to 2.5 K without any application of external DC Bias and/or AC-field. The inclusion of Mn at Ti site also enhances the ferromagnetic interaction for Dy2_2Ti1.8_{1.8}Mn0.2_{0.2}O7_7 as compared to Dy2_2Ti2_2O7_7. Arrhenius fit of freezing temperature with frequency for Dy2_2Ti1.8_{1.8}Mn0.2_{0.2}O7_7 shows that these spin relaxations at Ti_i and T\textless Ti_i are thermally induced. Low-temperature structural change in lattice parameters and crystal field phonon coupling has been studied using synchrotron x-ray diffraction. Debye-Gruineisen analysis of temperature-dependent lattice volume shows the emergence of crystal field phonon coupling at a much higher temperature (70 K) in Dy2_2Ti1.8_{1.8}Mn0.2_{0.2}O7_7 in contrast to 40 K in Dy2_2Ti2_2O7_7. These findings make Dy2_2Ti1.8_{1.8}Mn0.2_{0.2}O7_7 a suitable system to explore the application of the spin ice phenomenon at a workable temperature.

Explore this paper’s authors, topics and related work.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Reviews 0

Write a reviewWrite

No reviews yet.

Discussion 0

Add a commentWrite

No comments yet.