Abstract
As the need for miniaturized structural and functional materials has increased,the need for precise materials characterizaton has also expanded. Nanoindentation is a popular method that can be used to measure material mechanical behavior which enables high-throughput experiments and, in some cases, can also provide images of the indented area through scanning. Both indenting and scanning can cause tip wear that can influence the measurements. Therefore, precise characterization of tip radii is needed to improve data evaluation. A data fusion method is introduced which uses finite element simulations and experimental data to estimate the tip radius in situ in a meaningful way using an interpretable multi-fidelity deep learning approach. By interpreting the machine learning models, it is shown that the approaches are able to accurately capture physical indentation phenomena.
Connections
Explore this paper’s authors, topics and related work.
Building this map preview
BZPEER is loading the nearby papers, people, topics and institutions for this page.
Reviews 0
Write a review
No reviews yet.
Discussion 0
Add a comment
No comments yet.