Source author record

Tanmay Sarkar Akash

Tanmay Sarkar Akash appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.

ResearcherUnclaimed source record

Catalog footprint

What is connected

4works
1topics
4close collaborators

Actions

Connect this record

Log in to claim

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

4 published item(s)

preprint2020arXiv

Atomic Scale Insights Into The Mechanical Characteristics of Monolayer 1T-Titanium Disulphide: A Molecular Dynamics Study

In this work, we report on the mechanical responses and fracture behavior of pristine and defected monolayer 1T-Titanium Disulfide using classical molecular dynamics simulation. We investigated the effect of temperature, strain rate and defect ratio on the uniaxial tensile properties in both armchair and zigzag direction. We found that monolayer TiS2 shows isotropic uniaxial tensile properties except for failure strain which is greater in zigzag direction than armchair direction. We also observed a negative correlation of ultimate tensile strength, failure strain and young's modulus with temperature and defect ratio. Results depicts that strain rate has no effect on the young's modulus of monolayer TiS2 but higher strain rate results in higher ultimate tensile strength and failure strain.

preprint2020arXiv

Engineered Defects to Modulate Fracture Strength of Single Layer MoS2: An Atomistic Study

We use classical molecular dynamics (MD) simulations to investigate the mechanical properties of pre-cracked, nano-porous single layer MoS2 (SLMoS2) and the effect of interactions between cracks and pores. We found that the failure of pre-cracked and nano-porous SLMoS2 is dominated by brittle type fracture. Bonds in armchair direction show a stronger resistance to crack propagation compared to the zigzag direction. We compared the brittle failure of Griffith prediction with the MD fracture strength and toughness and found substantial differences that limit the applicability of Griffith criterion for SLMoS2 in case of nano-cracks and pores. Next, we demonstrate that the mechanical properties of pre-cracked SLMoS2 can be enhanced via symmetrically placed pores and auxiliary cracks around a central crack and position of such arrangements can be optimized for maximum enhancement of strengths. Such a study would help towards strain engineering based advanced designing of SLMoS2 and other similar Transition Metal Dichalcogenides.

preprint2020arXiv

Mechanical Properties and Fracture Phenomenon of Defected Monolayer Indium Selenide: A Molecular Dynamics Study

In this study, we report the mechanical properties and fracture mechanism of pre-cracked and defected InSe nanosheet samples using molecular dynamics (MD) simulations. We noticed that the failure of pre-cracked and defected InSe nanosheet is governed by brittle type fracture. Armchair directional bonds exhibit a greater resistance for crack propagation relative to the zigzag directional ones. Thus, fracture strength of the pre-cracked sheet is slightly higher for zigzag directional loading than that for armchair. We evaluated the limitation of the applicability of Griffith's criterion for single layer (SL) InSe sheet for nano-cracks as the brittle failure of Griffith prediction demonstrates significant differences with the MD fracture strength. We inspected the effect of temperature on the mechanical properties of the pre-cracked samples of SLInSe. We also discussed the fracture mechanism of both defected and pre-cracked structure at length.

preprint2020arXiv

Nanomechanics of Antimonene Allotropes

Monolayer antimonene has drawn the attention of research communities due to its promising physical properties. But mechanical properties of antimonene is still largely unexplored. In this work, we investigate the mechanical properties and fracture mechanisms of two stable phases of monolayer antimonene -- the $α$ antimonene ($α$-Sb) and the $β$ antimonene ($β$-Sb), through molecular dynamics (MD) simulations. Our simulations reveal that stronger chiral effect results in a greater anisotropic elastic behavior in $β$-antimonene than in $α$-antimonene. In this paper we focus on crack-tip stress distribution using local volume averaged virial stress definition and derive the fracture toughness from the crack-line stress. Our calculated crack tip stress distribution ensures the applicability of linear elastic fracture mechanics (LEFM) for cracked antimonene allotropes with considerable accuracy up to a pristine structure. We evaluate the effect of temperature, strain rate, crack-length and point-defect concentration on the strength and elastic properties. Tensile strength goes through significant degradation with the increment of temperature, crack length and defect percentage. Elastic modulus is less susceptible to temperature variation but is largely affected by the defect concentration. Strain rate induces a power law relation between strength and fracture strain. Finally, we discuss the fracture mechanisms in the light of crack propagation and establish the links between the fracture mechanism and the observed anisotropic properties.