Researcher profile

Jung In Yang

Jung In Yang contributes to research discovery and scholarly infrastructure.

ResearcherAffiliation not importedOpen to collaborate

Trust snapshot

Quick read

Trust 11 - UnverifiedVerification L1Unclaimed author
1works
0followers
2topics
4close collaborators

Actions

Decide how to stay connected

Follow researcher0

Identity and collaboration

How to connect with this researcher

Claiming links this public author record to a researcher profile and unlocks direct collaboration workflows.

Log in to claim

Direct collaboration

Open a focused conversation when the fit is right

Claim this author entity first to unlock direct invitations.

Research graph

See the researcher in context

Open full explorer

Inspect adjacent work, topics, institutions and collaborators without jumping out to a separate graph page.

Building this graph slice

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

1 published item(s)

preprint2022arXiv

Unique Ferroelectric Fatigue Behavior and Exceptional High Temperature Retention in Al0.93B0.07N Films

This paper reports the fatigue and retention behavior for Al1-xBxN thin films, a member of the novel family of wurtzite ferroelectrics, with an emphasis on the role of capacitor architecture. By modifying the capacitor architecture, and thus thermal and electrical boundary conditions, we create insight regarding the relative importance of intrinsic and extrinsic contributors to the degradation tendencies. Our experiments suggest that bipolar cycling of metal (Pt/W)/Al0.93B0.07N/W/Al2O3 film stacks first induced wake-up, then a region of constant switchable polarization. On additional cycling, the film leakage current increased, and then films underwent dielectric breakdown. For unpatterned first generation Al0.93B0.07N films with 100 nm thick Pt top electrodes survive ~104 bipolar cycles, whereas films with 1000 nm W top electrodes survive ~10^5 cycles before thermal dielectric breakdown. Sentaurus modeling was used to design an SU8 field plate which improved the performance to ~10^6 fatigue cycles. It was found that the thermal failures during fatigue were not due to surface flashover events but were associated with hard breakdown events in the dielectric. The films showed excellent retention of the stored polarization state. As expected, data retention was slightly inferior in the opposite state (OS) measurements. However, it is noted that even after 3.6x10^6 sec (1000 hr). at 200°C, the OS signal margin still exceeded 200 uC/cm2. The predicted OS retention is 82% after 10 years baking at 200oC.