Researcher profile

Johannes Feldl

Johannes Feldl contributes to research discovery and scholarly infrastructure.

ResearcherAffiliation not importedOpen to collaborate

Trust snapshot

Quick read

Trust 17 - UnverifiedVerification L1Unclaimed author
4works
0followers
2topics
4close collaborators

Actions

Decide how to stay connected

Follow researcher0

Identity and collaboration

How to connect with this researcher

Claiming links this public author record to a researcher profile and unlocks direct collaboration workflows.

Log in to claim

Direct collaboration

Open a focused conversation when the fit is right

Claim this author entity first to unlock direct invitations.

Research graph

See the researcher in context

Open full explorer

Inspect adjacent work, topics, institutions and collaborators without jumping out to a separate graph page.

Building this graph slice

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

4 published item(s)

preprint2020arXiv

Plasma-assisted molecular beam epitaxy of NiO on GaN(00.1)

The growth of NiO on GaN(00.1) substrates by plasma-assisted molecular beam epitaxy under oxygen rich conditions was investigated at growth temperatures between 100 $^{\circ}$C and 850 $^{\circ}$C. Epitaxial growth of NiO(111) with two rotational domains, with epitaxial relation $\normalsize{}\mathrm{\mathrm{\mathrm{NiO}(1\bar{\mathrm{1}}0)}\:||\:\mathrm{\mathrm{GaN}(11.0)}}$ and $\mathrm{\mathrm{\mathrm{NiO}\mathrm{(10\bar{\mathrm{1}})}\:||\:\mathrm{GaN(11.0)}}}$, was observed by X-ray diffraction (XRD) and confirmed by in-situ reflection high-energy electron diffraction as well as transmission electron microscopy (TEM) and electron backscatter diffraction. With respect to the high lattice mismatch of 8.1 % and a measured low residual tensile layer strain, growth by lattice matching epitaxy or domain matching epitaxy is discussed. The morphology measured by atomic force microscopy showed a grainy surface, probably arising from the growth by the columnar rotational domains visible in TEM micrographs. The domain sizes measured by AFM and TEM increase with the growth temperature, indicating an increasing surface diffusion length. Growth at 850 $^{\circ}$C, however, involved local decomposition of the GaN substrate that lead to an interfacial $\mathrmβ$-Ga$\mathrm{_{2}}$O$\mathrm{_{3}}$($\bar{\mathrm{2}}$01) layer and a high NiO surface roughness. Raman mesurements of the quasi-forbidden one-phonon peak indicate increasing layer quality (decreasing defect density) with increasing growth temperature. The results above suggest optimum growth temperatures around 700 $^{\circ}$C for high layer and interface quality.

preprint2020arXiv

Plasma-assisted molecular beam epitaxy of SnO(001) films: Metastability, hole transport properties, Seebeck coefficient, and effective hole mass

Transparent conducting or semiconducting oxides are important materials for (transparent) optoelectronics and power electronics applications. While most of these oxides can be doped n-type only with room-temperature electron mobilities on the order of 100cm^2/Vs p-type oxides are needed for the realization of pn-junction devices but typically suffer from exessively low (<<1cm^2/Vs) hole mobilities. Tin monoxide (SnO) is one of the few p-type oxides with a higher hole mobility, lacking a well-established understanding of its hole transport properties. Moreover, growth of SnO is complicated by its metastability with respect to SnO2 and Sn, requiring epitaxy for the realization of single crystalline material typically required for high-end applications. Here, we give a comprehensive account on the epitaxial growth of SnO, its (meta)stability, and its thermoelectric transport properties in the context of the present literature. Textured and single-crystalline, unintentionally-doped p-type SnO(001) films are grown by plasma-assisted molecular beam epitaxy. The metastability of this semiconducting oxide is addressed theoretically through an equilibrium phase diagram. Experimentally, the related SnO growth window is rapidly determined by an in-situ growth kinetics study as function of Sn-to-O-plasma flux ratio and growth temperature. The presence of secondary Sn and SnOx (1 < x <= 2) phases is comprehensively studied by different methods, indicating the presence of Sn3O4 or Sn as major secondary phases, as well as a fully oxidized SnO2 film surface. The hole transport properties, Seebeck coefficient, and density-of-states effective mass are determined and critically discussed in the context of the present literature on SnO, considering its anisotropic hole-effective mass.

preprint2020arXiv

Structural, optical, and electrical properties of unintentionally doped NiO layers grown on MgO by plasma-assisted molecular beam epitaxy

NiO layers were grown on MgO(100), MgO(110), and MgO(111) substrates by plasma-assisted molecular beam epitaxy under Ni-flux limited growth conditions. Single crystalline growth with a cube-on-cube epitaxial relationship was confirmed by X-ray diffraction measurements for all used growth conditions and substrates except MgO(111). A detailed growth series on MgO(100) was prepared using substrate temperatures ranging from 20 °C to 900 °C to investigate the influence on the layer characteristics. Energy-dispersive X-ray spectroscopy indicated close-to-stoichiometric layers with an oxygen content of ~47 at. % and ~50 at. % grown under low and high O-flux, respectively. All NiO layers had a root-mean-square surface roughness below 1 nm, measured by atomic force microscopy, except for rougher layers grown at 900 °C or using molecular oxygen. Growth at 900 °C led to a significant diffusion of Mg from the substrate into the film. The relative intensity of the quasi-forbidden one-phonon Raman peak is introduced as a gauge of the crystal quality, indicating the highest layer quality for growth at low oxygen flux and high growth temperature, likely due to the resulting high adatom diffusion length during growth. The optical and electrical properties were investigated by spectroscopic ellipsometry and resistance measurements, respectively. All NiO layers were transparent with an optical bandgap around 3.6 eV and semi-insulating at room temperature. However, changes upon exposure to reducing or oxidizing gases of the resistance of a representative layer at elevated temperature were able to confirm p-type conductivity, highlighting their suitability as a model system for research on oxide-based gas sensing.

preprint2019arXiv

Signatures of free carriers in Raman spectra of cubic In$_2$O$_3$

We discuss the influence of free carriers on the Raman scattering in $n$-type In$_2$O$_3$. For high-quality cubic single crystals, electronic single-particle excitations are revealed as a relatively broad Raman feature in the frequency range below 300~cm$^{-1}$. Furthermore, discrete phonon lines in the same frequency range exhibit asymmetric lineshapes characteristic for Fano resonances. The two observed spectral features contain the potential to be utilized for the quantitative determination of the free carrier concentration in $n$-type In$_2$O$_3$ using Raman spectroscopy as a contactless experimental technique.