Researcher profile

Jean Geringer

Jean Geringer contributes to research discovery and scholarly infrastructure.

ResearcherAffiliation not importedOpen to collaborate

Trust snapshot

Quick read

Trust 21 - EmergingVerification L1Unclaimed author
6works
0followers
2topics
4close collaborators

Actions

Decide how to stay connected

Follow researcher0

Identity and collaboration

How to connect with this researcher

Claiming links this public author record to a researcher profile and unlocks direct collaboration workflows.

Log in to claim

Direct collaboration

Open a focused conversation when the fit is right

Claim this author entity first to unlock direct invitations.

Research graph

See the researcher in context

Open full explorer

Inspect adjacent work, topics, institutions and collaborators without jumping out to a separate graph page.

Building this graph slice

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

6 published item(s)

preprint2014arXiv

Predicting the steady state thickness of passive films in order to prevent degradations of implant

Some implants have approximately a lifetime of 15 years. The femoral stem, for example, should be made of 316L/316LN stainless steel. Fretting corrosion, friction under small displacements, should occur during human gait, due to repeated loadings and un-loadings, between stainless steel and bone for instance. Some experimental investigations of fretting corrosion have been practiced. As well known, metallic alloys and especially stainless steels are covered with a passive film that prevents from the corrosion and degradation. This passive layer of few nanometers, at ambient temperature, is the key of our civilization according to some authors. This work is dedicated to predict the passive layer thicknesses of stainless steel under fretting corrosion with a specific emphasis on the role of proteins. The model is based on the Point Defect Model (micro scale) and an update of the model on the friction process (micro-macro scale). Genetic algorithm was used for finding solution of the problem. The major results are, as expected from experimental results, albumin prevents from degradation at the lowest concentration of chlorides; an incubation time is necessary for degrading the passive film; under fretting corrosion and high concentration of chlorides the passive behavior is annihilated.

preprint2013arXiv

Degradation of alumina and zirconia toughened alumina (ZTA) hip prostheses tested under microseparation conditions in a shock device

This paper considers the degradation of alumina and zirconia toughened alumina vs. alumina for hip implants. The materials are as assumed to be load bearing surfaces subjected to shocks in wet conditions. The load is a peak of force; 9 kN was applied over 15 ms at 2 Hz for 800,000 cycles. The volumetric wear and roughness are lower for ZTA than for alumina. The long ZTA ageing did not seem to have a direct influence on the roughness. The ageing increased the wear volumes of ZTA and it was found to have a higher wear resistance compared to alumina.

preprint2013arXiv

Fracture simulation for zirconia toughened alumina microstructure

Purpose - The purpose of this paper is to describe finite element modelling for fracture and fatigue behaviour of zirconia toughened alumina microstructures. Design/methodology/approach - A two-dimensional finite element model is developed with an actual $Al{_2}O{_3}$ - 10 vol% $ZrO{_2}$ microstructure. A bilinear, time-independent cohesive zone law is implemented for describing fracture behaviour of grain boundaries. Simulation conditions are similar to those found at contact between a head and a cup of hip prosthesis. Residual stresses arisen from the mismatch of thermal coefficient between grains are determined. Then, effects of a micro-void and contact stress magnitude are investigated with models containing residual stresses. For the purpose of simulating fatigue behaviour, cyclic loadings are applied to the models. Findings - Results show that crack density is gradually increased with increasing magnitude of contact stress or number of fatigue cycles. It is also identified that a micro-void brings about the increase of crack density rate. Social implications - This paper is the first step for predicting the lifetime of ceramic implants. The social implications would appear in the next few years about health issues. Originality/value - This proposed finite element method allows describing fracture and fatigue behaviours of alumina-zirconia microstructures for hip prosthesis, provided that a microstructure image is available.

preprint2013arXiv

Predicting the steady state thickness of passive films with the Point Defect Model in fretting corrosion experiments

Some implants have approximately a lifetime of 15 years. The femoral stem, for example, should be made of 316L/316LN stainless steel. Fretting corrosion, friction under small displacements, should occur during human gait, due to repeated loadings and un-loadings, between stainless steel and bone for instance. Some experimental investigations of fretting corrosion have been practiced. As well known, metallic alloys and especially stainless steels are covered with a passive film that prevents from the corrosion and degradation. This passive layer of few nanometers, at ambient temperature, is the key of our civilization according to some authors. This work is dedicated to predict the passive layer thicknesses of stainless steel under fretting corrosion with a specific emphasis on the role of proteins. The model is based on the Point Defect Model (micro scale) and an update of the model on the friction process (micro-macro scale). Genetic algorithm was used for finding solution of the problem. The major results are, as expected from experimental results, albumin prevents from degradation at the lowest concentration of chlorides; an incubation time is necessary for degrading the passive film; under fretting corrosion and high concentration of chlorides the passive behavior is annihilated. Les implants orthopédiques de hanche ont une durée de vie d'environ 15 ans. Par exemple, la tige fémorale d'un tel implant peut être réalisée en acier inoxydable 316L ou 316LN. Le fretting corrosion, frottement sous petits déplacements, peut se produire pendant la marche humaine en raison des chargements répétés entre le métal de la prothèse et l'os. Plusieurs investigations expérimentales du fretting corrosion ont été entreprises. Cette couche passive de quelques nanomètres, à température ambiante, est le point clef sur lequel repose le développement de notre civilisation, selon certains auteurs. Ce travail vise à prédire les épaisseurs de cette couche passive de l'acier inoxydable soumis au fretting corrosion, avec une attention spécifique sur le rôle des protéines. Le modèle utilisé est basé sur le Point Defect Model, PDM (à une échelle microscopique) et une amélioration de ce modèle en prenant en compte le processus de frottement sous petits débattements. L'algorithme génétique a été utilisé pour optimiser la convergence du problème. Les résultats les plus importants sont, comme démontré avec les essais expérimentaux, que l'albumine, la protéine étudiée, empêche les dégradations de l'acier inoxydable aux plus faibles concentrations d'ions chlorure ; ensuite, aux plus fortes concentrations de chlorures, un temps d'incubation est nécessaire pour détruire le film passif.

preprint2012arXiv

Finite element modelling of shock-induced damages on ceramic hip prostheses

The aim of this work was to simulate the behaviour of hip prostheses under mechanical shocks. When hip joint is replaced by prosthesis, during the swing phase of the leg, a microseparation between the prosthetic head and the cup could occur. Two different sizes of femoral heads were studied: 28 and 32 mm diameter, made, respectively, in alumina and zirconia. The shock-induced stress was determined numerically using finite element analysis (FEA), Abaqus software. The influence of inclination, force, material, and microseparation was studied. In addition, an algorithm was developed from a probabilistic model, Todinov's approach, to predict lifetime of head and cup. Simulations showed maximum tensile stresses were reached on the cup's surfaces near to rim. The worst case was the cup-head mounted at 30^{\circ}. All simulations and tests showed bulk zirconia had a greater resistance to shocks than bulk alumina. The probability of failure could be bigger than 0.9 when a porosity greater than 0.7% vol. is present in the material. Simulating results showed good agreement with experimental results. The tests and simulations are promising for predicting the lifetime of ceramic prostheses.

preprint2010arXiv

Influence of proteins from physiological solutions on the electrochemical behaviour of the Ti-6Al-4V alloy: reproducibility and time-frequency dependence. ---- Influence de la teneur en protéines de solutions physiologiques sur le comportement électrochimique du Ti-6Al-4V : reproductibilité et représentation temps-fréquence

The electrochemical behaviour of the biomedical and metallic alloys, especially in the orthopaedic implants fields, raises many questions. This study is dedicated for studying the Ti-6Al-4V alloy, by electrochemical impedance spectroscopy, EIS, in various physiological media,: Ringer solution, phosphate buffered solution (PBS), PBS solution and albumin, PBS solution with calf serum and PBS solution with calf serum and an antioxidant (sodium azide). Moreover, the desionised water was considered as the reference solution. The tests reproducibility was investigated. The time-frequency-Module graphs highlighted that the desionised water is the most protective for the Ti-6Al-4V alloy. This biomedical alloy is the less protected in the solution constituted by PBS and albumin. The time-frequency graph allows pointing out the graphic signatures of adsorption for organic and inorganic species (differences between the modules means in studied solution and the modules mean in the reference solution). --- Le comportement électrochimique des alliages métalliques biomédicaux, notamment dans le domaine des implants orthopédiques, pose encore de nombreuses questions. Ce travail propose d'étudier l'alliage de titane Ti-6Al-4V, par spectroscopie d'impédance électrochimique, SIE, dans différents milieux physiologiques : solution de Ringer, solution à base d'un tampon phosphate (PBS), solution PBS avec de l'albumine, solution PBS avec du sérum bovin et une solution PBS avec du sérum bovin et un antioxydant (azoture de sodium). De plus, une solution d'eau ultra-pure servira de référence. La reproductibilité des tests a été étudiée. Les représentations temps-fréquence des modules ont mis en évidence que l'eau désionisée est la solution qui présente le caractère le plus protecteur pour le Ti-6Al-4V. Cet alliage de titane est le moins protégé dans la solution de PBS contenant de l'albumine. Cette représentation permet de mettre en évidence des signatures graphiques d'adsorption des espèces inorganiques et organiques (différences entre les moyennes des modules dans les solutions étudiées et la moyenne des modules dans la solution de référence).