Source author record

Dongliang Wang

Dongliang Wang appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.

ResearcherUnclaimed source record

Catalog footprint

What is connected

38works
4topics
4close collaborators

Actions

Connect this record

Log in to claim

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

38 published item(s)

preprint2022arXiv

AGENT: An Adaptive Grouping Entrapping Method of Flocking Systems

This study proposes a distributed algorithm that makes agents' adaptive grouping entrap multiple targets via automatic decision making, smooth flocking, and well-distributed entrapping. Agents make their own decisions about which targets to surround based on environmental information. An improved artificial potential field method is proposed to enable agents to smoothly and naturally change the formation to adapt to the environment. The proposed strategies guarantee that the coordination of swarm agents develops the phenomenon of multiple targets entrapping at the swarm level. We validate the performance of the proposed method using simulation experiments and design indicators for the analysis of these simulation and physical experiments.

preprint2020arXiv

Collaborative Distillation in the Parameter and Spectrum Domains for Video Action Recognition

Recent years have witnessed the significant progress of action recognition task with deep networks. However, most of current video networks require large memory and computational resources, which hinders their applications in practice. Existing knowledge distillation methods are limited to the image-level spatial domain, ignoring the temporal and frequency information which provide structural knowledge and are important for video analysis. This paper explores how to train small and efficient networks for action recognition. Specifically, we propose two distillation strategies in the frequency domain, namely the feature spectrum and parameter distribution distillations respectively. Our insight is that appealing performance of action recognition requires \textit{explicitly} modeling the temporal frequency spectrum of video features. Therefore, we introduce a spectrum loss that enforces the student network to mimic the temporal frequency spectrum from the teacher network, instead of \textit{implicitly} distilling features as many previous works. Second, the parameter frequency distribution is further adopted to guide the student network to learn the appearance modeling process from the teacher. Besides, a collaborative learning strategy is presented to optimize the training process from a probabilistic view. Extensive experiments are conducted on several action recognition benchmarks, such as Kinetics, Something-Something, and Jester, which consistently verify effectiveness of our approach, and demonstrate that our method can achieve higher performance than state-of-the-art methods with the same backbone.

preprint2016arXiv

Vortex pinning and dynamics in high performance Sr0.6K0.4Fe2As2 superconductor

We have studied vortex pinning and dynamics in a Sr0.6K0.4Fe2As2 superconducting tape with critical current density Jc~0.1 MA/cm2 at 4.2 K and 10 T. It is found that grain boundary pinning is dominant in the vortex pinning mechanism. Furthermore, we observe large density of dislocations which can also serve as effective pinning centers. We find that the temperature dependence of critical current density is in agreement with the model of vortices pinned via spatial fluctuation of charge carrier mean free path. Magnetic relaxation measurement indicates that the magnetization depends on time in a logarithmic way. The relaxation rate in the low and intermediate temperature region is small, and it exhibits a weak temperature and field dependence. A crossover from elastic creep to plastic creep regime is observed. Finally, we conclude a vortex phase diagram for the high performance Sr0.6K0.4Fe2As2 superconducting tape.

preprint2015arXiv

High performance FeSe0.5Te0.5 thin films grown at low temperature by pulsed laser deposition

We report on fully epitaxial FeSe0.5Te0.5 (FST) thin films with high-quality grown on CaF2 (00l) substrate at a low temperature of 300°C by pulsed laser deposition. The transport Jc of thin films is up to 1.36 MA/cm2 in self-field and 0.97 MA/cm2 in 9 T at 4.2 K, indicating very weak field dependence. A nearly isotropy of Jc (γ= Jc(H//ab)/Jc(H//c) as low as 1.09 at 9 T is achieved in the FST thin films. Moreover, no clear amorphous interfacial layer presents between the film and the substrate probably ascribing to low temperature and low laser repetition rate grown, while the thickness of reaction layer is approximate 5 nm in many other works. The evidences of transmission electron microscopy show some lattices with lateral size of < 5 nm x 20 nm seem to be disturbed. Those location defects are thought to be responsible for nearly isotropic behavior of superconductivity.

preprint2015arXiv

Large transport Jc in Cu-sheathed Sr0.6K0.4Fe2As2 superconducting tape conductors

Copper sheath is the first choice for manufacturing high-Tc superconducting wires and tapes because of its high electrical and thermal conductivities, low cost and good mechanical properties. However, Cu can easily react with superconducting cores, such as BSCCO, MgB2 and pnictides, during high-temperature sintering process and therefore drastically decrease the transport Jc. Here, we report the fabrication of Cu-sheathed Sr1-xKxFe2As2 tapes with superior Jc performance using a simple hot pressing method that is capable of eliminating the lengthy high-temperature sintering required by conventional process. We obtained high-quality Sr1-xKxFe2As2 tapes with processing at 800oC for 30 minutes and measured high Tc and sharp transition. This rapid fabrication method can effectively thwart the diffusion of Cu into polycrystalline Sr-122 core. As a consequence, we achieved high transport Jc of 3.1x10^4 A/cm^2 in 10 T and 2.7x10^4 A/cm^2 in 14 T at 4.2 K. The in-field Jc performance is by far the highest reported for Cu-sheathed high-Tc conductors. Our results demonstrate the potential of Cu sheath for practical application of pnictide wires and tapes.

preprint2014arXiv

Enhancement of transport critical current density of SmFeAsO1-xFx tapes fabricated by an ex-situ powder-in-tube method with a Sn-presintering process

SmFeAsO1-xFx (Sm1111) tapes were prepared by an ex-situ powder-in-tube method with a Sn-presintering process. Scanning electron microscopy revealed apparent difference in microstructure between Sn-presintered tapes and the previously reported polycrystalline Sm1111 bulk, since Sn has reduced FeAs wetting phase and filled the voids between Sm1111 grains. The Sn-presintered tapes showed significant enhanced field dependences of transport Jc compared with Sn-added tapes. A highest transport critical current density (Jc) of 3.45x10^4 A cm-2 at 4.2 K and self-field is achieved. Magneto-optical (MO) imaging further confirmed large and well-distributed global and intergranular Jc in Sn-presintered Sm1111 tapes.

preprint2014arXiv

High critical current density in textured Ba-122/Ag tapes fabricated by scalable rolling process

The industrial manufacturing of the long-length iron-pnictide wires and tapes requires simple and low-cost technology. Although the transport critical current density of the FeAs-122 tapes has already achieved the practical application level, their fabrication procedures are relatively complicated or required specialized instruments. Ag-sheathed Ba0.6K0.4Fe2As2 superconducting tapes were fabricated by the scalable rolling process. At 4.2 K and 10 T, the critical current density Jc has achieved 5.4x10^4 A/cm2. We ascribe the excellent performance to the high purity and homogeneity of the superconducting phase, high density and high c-axis texture of the superconducting core. Our method provides a simple way to scale up the production of the long-length iron-based superconducting tapes with high Jc.

preprint2014arXiv

Hot pressing to enhance the transport Jc of Sr0.6K0.4Fe2As2 superconducting tapes

High-performance Sr0.6K0.4Fe2As2 (Sr-122) tapes have been successfully fabricated using hot pressing (HP) process. The effect of HP temperatures (850-925 C) on the c-axis texture, resistivity, Vickers micro-hardness, microstructure and critical current properties has been systematically studied. Taking advantage of high degree of c-axis texture, well grain connectivity and and large concentration of strong-pinning defects, we are able to obtain an excellent Jc of 1.2x10^5 A/cm^2 at 4.2 K and 10 T for Sr-122 tapes. More importantly, the field dependence of Jc turns out to be very weak, such that in 14 T the Jc remains ~1.0x10^5 A/cm^2. These Jc values are the highest ever reported so far for iron-pnictide wires and tapes, achieving the level desired for practical applications. Our results clearly strengthen the position of iron-pnictide conductors as a competitor to the conventional and MgB2 superconductors for high field applications.

preprint2014arXiv

Realization of practical level current densities in Sr0.6K0.4Fe2As2 tape conductors for high-field applications

122 type pnictide superconductors are of particular interest for high-field applications because of their large upper critical fields Hc2 (> 100 T), low Hc2 anisotropy r (< 2), and high thin-film critical current densities Jc (> 1 MA/cm2 at 4.2 K). Successful magnet applications require fabrication of polycrystalline superconducting wires that exhibit large in-field Jc, which is limited by poor grain coupling and weak-link behavior at grain boundaries. Here we report our recent achievement in the developing Sr0.6K0.4Fe2As2 tapes with transport Jc up to 0.1 MA/cm2 at 10 T and 4.2 K. This value is by far the highest ever recorded for iron based superconducting wires and has surpassed the threshold for practical application for the first time. The synergy effects of enhanced grain connectivity, alleviation of the weak-link behavior at grain boundaries, and the strong intrinsic pinning characteristics led to the superior Jc performance exhibited in our samples. This advanced Jc result opens up the possibility for iron-pnictide superconducting wires to win the race in high-field magnet applications.

preprint2014arXiv

Strongly enhanced current densities in Sr0.6K0.4Fe2As2 superconducting tapes

Improving transport current has been the primary issue for practical application of superconducting wires and tapes. However, the porous nature of powder-in-tube (PIT) processed iron-based superconducting tapes is thought to be one of the important reasons for the low Jc values. In this work, the superconducting core density of ex-situ Sr0.6K0.4Fe2As2 tapes was significantly improved by employing a simple hot pressing as an alternative route for final sintering. At 4.2 K, the transport Jc values showed excellent values of 5.1x10^4 A/cm^2 at 10 T and 4.3x10^4 A/cm^2 at 14 T, respectively, which attain the Jc level desired for practical applications. Moreover, the Jc values exhibited extremely weak magnetic field dependence. These results clearly demonstrate that PIT pnictide wire conductors are very promising for high field magnet applications.

preprint2013arXiv

High critical current density and low anisotropy in textured Sr1-xKxFe2As2 tapes for high field applications

From the application point of view, large critical current densities Jc (H) for superconducting wires are required, preferably for magnetic fields higher than 5 T. Here we show that strong c-axis textured Sr1-xKxFe2As2 tapes with nearly isotropic transport Jc were fabricated by an ex-situ powder-in-tube (PIT) process. At 4.2 K, the Jc values show extremely weak magnetic field dependence and reach high values of 1.7x10^4 A/cm^2 at 10 T and 1.4x10^4 A/cm^2 at 14 T, respectively, these values are by far the highest ever reported for iron based wires and approach the Jc level desired for practical applications. Transmission electron microscopy investigations revealed that amorphous oxide layers at grain boundaries were significantly reduced by Sn addition which resulted in greatly improved intergranular connectivity. Our results demonstrated the strong potential of using iron based superconductors for high field applications.

preprint2013arXiv

Large transport critical currents and magneto-optical imaging of textured Sr1-xKxFe2As2 superconducting tapes

We report the temperature dependence of the transport critical current density (Jc) in textured Sr1-xKxFe2As2/Fe (Sr122) tapes fabricated by an ex situ powder-in-tube process. Critical currents were measured in magnetic fields up to 0-15 T and/or the temperature range 4.2-30 K by using a dc four-probe method. It was found that textured Sr122 tapes heat-treated at low temperatures showed higher transport Jc performance due to much improved intergrain connections. At temperatures of 20 K, easily obtained using a cryocooler, Jc reached ~ 10^4 A/cm^2 in self field, which is the highest transport value of ferropnictide wires and tapes reported so far. Magneto-optical imaging observations further revealed significant and well distributed global Jc at 20 K in our tapes. These results demonstrate that 122 type superconducting tapes are promising for high-field applications at around 20 K.

preprint2012arXiv

Calculation of the transport critical current density of c-axis textured 122 iron-based superconductors

The c-axis textured Sr1-xKxFe2As2 tapes produced by cold rolling and post-annealing, could carry a high super-current over 2*104 A/cm2. However, the magnitude is far from its maximum, because of the current obstacles associated with various defects in the material. To predict the maximal transport critical current density, we modeled the current paths in a c-axis textured polycrystal as a three-dimensional flow network, and calculated the maximum flow with the Ford-Fulkerson algorithm. It indicates that a much higher super-current of about 2*105 A/cm2 could be achieved in an ideal c-axis textured K-doped 122 polycrystal. The dependences of transport Jc on density, content of invalid boundary and grain size and shape were also studied. The results imply that, over 30% of the grain boundaries in the reported c-axis textured Sr1-xKxFe2As2 tapes may act as current obstacles, and the large ratio of width to thickness was expected to be the most favorable grain shape for high transport Jc in c-axis textured 122 superconducting tapes.

preprint2012arXiv

Effect of starting materials on the superconducting properties of SmFeAsO1-xFx tapes

SmFeAsO1-xFx tapes were prepared using three kinds of starting materials. It shows that the starting materials have an obvious effect on the impurity phases in final superconducting tapes. Compared with the other samples, the samples fabricated by SmAs, FeO, Fe2As, and SmF3 have the smallest arsenide impurity phase and voids. As a result, these samples possess much denser structure and better grain connectivity. Moreover, among the three kinds of samples fabricated in this work, this kind of sample has the highest zero-resistivity temperature ~40 K and largest critical current density ~4600 A/cm^2 in self-field at 4.2 K. This is the highest Jc values reported so far for SmFeAsO1-xFx wires and tapes.

preprint2012arXiv

Fabrication and transport properties of Sr0.6K0.4Fe2As2 multifilamentary superconducting wires

Seven-core Ag/Fe sheathed Sr0.6K0.4Fe2As2 (Sr-122) superconducting wires were produced by the ex situ powder-in-tube (PIT) method. The relationship between the cold-work deformation process and the superconducting properties of wires were systematically studied. It was found that flat rolling can efficiently increase the density of the superconducting core and largely improve the transport critical current density (Jc) of as-drawn wires. The Jc of the best sample achieved 21.1 kA/cm^2 at 4.2 K in self field, and showed very weak magnetic field dependence in high fields. Our result suggested a promising future of multifilamentary iron-based superconductors in practical application.

preprint2012arXiv

Improved transport critical currents in Ag and Pb co-doped BaxK1-xFe2As2 superconducting tapes

Fe-clad BaxK1-xFe2As2 superconducting tapes were fabricated by the ex situ powder-in-tube method combined with a short high-temperature annealing technique. The effect of annealing time and different dopants on the transport properties of the BaxK1-xFe2As2 tapes were systematically studied. By co-doping with Ag and Pb, the transport critical current density Jc of BaxK1-xFe2As2 tapes was significantly improved in whole field region and the highest transport Jc was up to 1.4x10^4 A/cm^2 (Ic=100 A) at 4.2K in self field. It is proposed that the superior Jc in the co-doped samples are due to the combine effect of Pb doping at low fields and Ag doping at high fields.

preprint2011arXiv

Development of Powder-in-Tube Processed Iron Pnictide Wires and Tapes

The development of the PIT fabrication process of iron pnictide superconducting wires and tapes has been carried out in order to enhance their transport properties. Silver was found to be the best sheath material, since no reaction layer was observed between the silver sheath and the superconducting core. The grain connectivity of iron pnictide wires and tapes has been markedly improved by employing Ag or Pb as dopants. At present, critical current densities in excess of 3750 A/cm^2 (Ic = 37.5 A) at 4.2 K have been achieved on Ag-sheathed SrKFeAs wires prepared with the above techniques, which is the highest in iron-based wires and tapes so far. Moreover, Ag-sheathed Sm-1111 superconducting tapes were successfully prepared by PIT method at temperatures as low as 900C, instead of commonly used temperatures of 1200C. These results demonstrate the feasibility of producing superconducting pnictide composite wires, even grain boundary properties require much more attention.

preprint2011arXiv

Direct observation of nanometer-scale amorphous layers and oxide crystallites at grain boundaries in polycrystalline Sr1-xKxFe2As2 superconductors

We report here an atomic resolution study of the structure and composition of the grain boundaries in polycrystalline Sr0.6K0.4Fe2As2 superconductor. A large fraction of grain boundaries contain amorphous layers larger than the coherence length, while some others contain nanometer-scale particles sandwiched in between amorphous layers. We also find that there is significant oxygen enrichment at the grain boundaries. Such results explain the relatively low transport critical current density (Jc) of polycrystalline samples with respect to that of bicrystal films.

preprint2011arXiv

Enhanced critical current properties in Ba0.6K0.4+xFe2As2 superconductor by over-doping of potassium

Phase-pure polycrystalline Ba0.6K0.4+xFe2As2 with were prepared using a one-step solid-state reaction method. We found that over-doping of potassium can improve critical current density (Jc). High-field Jc for samples with x = 0.1 is three times higher than that for samples with x = 0. Over-doping of K has minimal effect on the critical transition temperature (Tc). Less than 0.5 K degradations in Tc was measured for samples with x = 0.1. TEM revealed high concentration of dislocations in samples with x = 0.1, resulting in enhanced flux pining. Further analyses on magnetization loops for powder samples confirm that K over-doping can promote intra-grain Jc. Our results indicate that slight excess of K in Ba0.6K0.4Fe2As2 samples is beneficial to high-field applications.

preprint2011arXiv

High transport critical current densities in textured Fe-sheathed Sr1-xKxFe2As2+Sn superconducting tapes

We report the realization of grain alignment in Sn-added Sr1-xKxFe2As2 superconducting tapes prepared by ex-situ powder-in-tube method. At 4.2 K, high transport critical current densities Jc of 2.5x10^4 A/cm^2 (Ic = 180 A) in self-field and 3.5x10^3 A/cm^2 (Ic = 25.5 A) in 10 T have been measured. These values are the highest ever reported so far for Fe-based superconducting wires and tapes. We believe the superior Jc in our tape samples are due to well textured grains and strengthened intergrain coupling achieved by Sn addition. Our results demonstrated an encouraging prospect for application of iron based superconductors.

preprint2011arXiv

Superconducting properties of FeSe wires and tapes prepared by gas diffusion technique

Superconducting FeSe in the form of wires and tapes were successfully fabricated using a novel gas diffusion procedure. Structural analysis by mean of x-ray diffraction shows that themain phase of tetragonal PbO-type FeSe was obtained by this synthesis method. The zero resistivity transition temperature of the FeSe was confirmed to be 9.3 K. The critical current density as high as 137 A/cm^2 (4 K, self field) has been observed. The results suggest that the diffusion procedure is promising in preparing high-quality FeSe wires and tapes.

preprint2011arXiv

Superconductivity induced by doping Rh in CaFe2-xRhxAs2

In this paper we report the synthesis of iron-based superconductors CaFe2-xRhxAs2 using one-step solid state reaction method, which crystallizes in the ThCr2Si2-type structure with a space group I4/mmm. The systematic evolution of the lattice constants demonstrates that the Fe ions are successfully replaced by the Rh. By increasing the doping content of Rh, the spin-density-wave (SDW) transition in the parent compound is suppressed and superconductivity emerges. The maximum superconducting transition temperature is found at 18.5 K with the doping level of x = 0.15. The temperature dependence of DC magnetization confirms superconducting transitions at around 15 K. The general phase diagram was obtained and found to be similar to the case of Rh-doping Sr122 system. Our results explicitly demonstrate the feasibility of inducing superconductivity in Ca122 compounds by higher d-orbital electrons doping, however, different Rh-doping effect between FeAs122 compounds and FeAs1111 systems still remains an open question.

preprint2011arXiv

Synthesis and properties of La-doped CaFe2As2 single crystals with Tc = 42.7 K

Large single crystals of La-doped CaFe2As2 were successfully synthesized by the FeAs self-flux method. The x-ray diffraction patterns suggest high crystalline quality and c-axis orientation. By substitution of trivalent La3+ ions for divalent Ca2+, the resistivity anomaly in the parent compound CaFe2As2 is completely suppressed and a superconducting transition reaches the value of 42.7 K, which is higher than that of about 30 K reported in Saha S. R. et al., arXiv:1105.4798v1. The upper critical field has been determined with the magnetic field along ab-plane and c-axis, yielding an anisotropy of about 3.3.

preprint2011arXiv

Transport properties and anisotropy in rare earth doped CaFe2As2 single crystals with Tc above 40 K

In this paper we report the superconductivity above 40 K in the electron doping single crystal Ca1-xRexFe2As2 (Re = La, Ce, Pr). The x-ray diffraction patterns indicate high crystalline quality and c-axis orientation. the resistivity anomaly in the parent compound CaFe2As2 is completely suppressed by partial replacement of Ca by rare earth and a superconducting transition reaches as high as 43 K, which is higher than the value in electron doping FeAs-122 compounds by substituting Fe ions with transition metal, even surpasses the highest values observed in hole doping systems with a transition temperature up to 38 K. The upper critical field has been determined with the magnetic field along ab-plane and c-axis, yielding the anisotropy of 2~3. Hall-effect measurements indicate that the conduction in this material is dominated by electron like charge carriers. Our results explicitly demonstrate the feasibility of inducing superconductivity in Ca122 compounds via electron doping using aliovalent rare earth substitution into the alkaline earth site, which should add more ingredients to the underlying physics of the iron-based superconductors.

preprint2011arXiv

Upper fields and critical current density of K0.58Fe1.56Se2 single crystals grown by one step technique

Single crystals of K0.58Fe1.56Se2 were successfully synthesized by a new single step process with the onset superconducting transition temperatures 31.9 K. The x-ray diffraction patterns suggest that they have high crystalline quality and c-axis orientation. A possible modulation structure of Fe-vacancy along c axis was observed. The upper critical field has been determined with the magnetic field along ab-plane and c-axis, yielding an anisotropy of about 3.3. It has also been shown that the critical current density of the K0.58Fe1.56Se2 is about 1.7x10^4 A/cm^2 at 5 K.

preprint2010arXiv

Development of Doped MgB2 Wires and Tapes for Practical Applications

A review of current developments in the study of chemical doping effect on the superconducting properties of MgB2 wires and tapes is presented, based on the known literature data and our own results. The critical current density of MgB2 can be improved through various kinds of dopants. Among these dopants, doping with carbon-containing materials seems to be the most effective way to improve the Jc performance. The doping effect of carbon in different forms and carbon-based compounds such as SiC, nano-C, metal carbides, as well as aromatic hydrocarbon and carbohydrate on the Jc-B characteristics of MgB2 was discussed in detail. The C can be incorporated into the MgB2 crystal lattice by replacing boron, and thus Bc2 is significantly enhanced due to selective tuning of impurity scattering of two bands in the two-band MgB2. Besides the efforts of increasing Bc2 by carbon doping, the fine grain size and nano-size inclusions caused by doping would create many flux pinning centres improving the Jc-B property of MgB2. Based on these considerations, we suggested some principles for the selection of dopants.

preprint2010arXiv

Fabrication and some properties of biaxially aligned Sr0.6K0.4Fe2As2 superconductors by processing in high magnetic field

We fabricated the c axis and ab-plane biaxially aligned Sr0.6K0.4Fe2As2 superconductor using a two-step magnetic field procedure. The effect of magnetic fields on the structure and superconducting properties of Sr0.6K0.4Fe2As2 has been investigated by using X-ray diffraction and magnetic measurements. The degree of orientation of the samples was about 0.39 for the c axis and 0.51 for ab-plane orientation, as evaluated from the Lotgering factor of X-ray diffraction. This technology might be useful in a variety of potential applications, including preparing iron based superconducting bulks and wires with high critical currents.

preprint2010arXiv

Heat treatment effects on the superconducting properties of Ag-doped SrKFeAs compound

The superconducting properties of polycrystalline Sr0.6K0.4Fe2As2 were strongly influenced by Ag doping (Supercond. Sci. Technol. 23 (2010) 025027). Ag addition is mainly dominated by silver diffusing, so the annealing process is one of the essential factors to achieve high quality Ag doped Sr0.6K0.4Fe2As2. In this paper, the optimal annealing conditions were studied for Ag doped Sr0.6K0.4Fe2As2 bulks prepared by a one-step solid reaction method. It is found that the annealing temperature has a strong influence on the superconducting properties, especially on the critical current density Jc. As a result, higher heat treatment temperature (~900C) is helpful in diffusing Ag and reducing the impurity phase gathered together to improve the grain connectivity. In contrast, low-temperature sintering is counterproductive for Ag doped samples. These results clearly suggest that annealing at ~900C is necessary for obtaining high Jc Ag-doped samples.

preprint2010arXiv

Influence of Pb addition on the superconducting properties of polycrystalline Sr0.6K0.4Fe2As2

Polycrystalline Sr0.6K0.4Fe2As2 samples with various Pb additions (0-20 wt%) were prepared using a one-step solid state reaction. X-ray diffraction analysis shows no evidence for chemical reaction between the Pb and the FeAs-based superconductor. However, the presence of the Pb can affect the microstructure and superconducting properties of the final products. The critical transition temperature Tc indicates no degradation up to 20 wt% Pb addition, and dramatic improvements of magnetic Jc and irreversibility field Hirr were observed for appropriate Pb concentration. Transport critical current property of pure and Pb-added Sr0.6K0.4Fe2As2 tapes was also measured by a four-probe technique, and a remarkable enhancement of Jc at low fields was detected for the Pb added tapes.

preprint2010arXiv

Low-temperature synthesis of SmFeAsO0.7F0.3 wires with high transport critical current density

Ag-sheathed SmFeAsO0.7F0.3 (Sm-1111) superconducting wires were prepared by a one-step solid state reaction at temperatures as low as 850~900C, instead of commonly used temperatures of 1150~1250C. The X-ray diffraction pattern of the as-sintered samples is well indexed on the basis of tetragonal ZrCuSiAs-type structure. We characterized transport critical current density Jc of the SmFeAsO0.7F0.3 wires in increasing and subsequently decreasing fields, by a resistive four-probe method. A transport Jc as high as ~1300 A/cm^2 at 4.2 K and self field has been observed for the first time in Sm-1111 type polycrystalline superconductors. The Jc also shows a rapid depression in small applied fields as well as a magnetic-history dependence, indicating weak-linked grain boundaries. The low-temperature synthesis method can be very beneficial to fabricating the RE-1111 iron oxynictides in a convenient and safe way.

preprint2010arXiv

Low-temperature synthesis of SmO0.8F0.2FeAs superconductor with Tc = 56.1K

We report a systematic study on the effect of sintering temperature on the structural and superconducting properties of nominal SmO0.8F0.2FeAs fabricated by simple one-step solid state reaction method. A detailed correlation between the sintering temperature, structure, onset transition temperature (Tc) and critical current density (Jc) has been found in all samples of each batch. Most importantly, samples sintered at a low temperature clearly shows high Tc, for example the Tc of the samples sintered at 850C is even above 53 K, and the samples prepared at 1000C display the highest Tc of 56.1 K reported so far. Furthermore, the samples sintered at 1000C also show the highest RRR and the lowest resistivity(57K), indicating the low impurity scattering and enhanced carrier density. However, the maximum Jc of 10510 A/cm^2 at 5 K in self field was achieved in the samples sintered at 1100oC. The dependence of Tc on a-axis lattice constant indicates that the sintering temperature has strong influence on the effective substitution level of F for O. This result suggests that annealing at a temperature of ~1000C seems much better for obtaining high quality 1111 phase oxypnictides, compared to commonly used temperatures of around 1200C.

preprint2010arXiv

One-step method to grow Ba0.6K0.4Fe2As2 single crystals without fluxing agent

Single crystals of Ba0.6K0.4Fe2As2 with excellent quality have been successfully grown without fluxing agent through a simple one-step method for the first time. X-ray diffraction patterns demonstrate that the samples have high crystalline quality and c-axis orientation. The onset transition temperature is up to 38 K with the zero resistivity temperature about 36.7 K. Both the R-T and M-T data show a very sharp superconducting transition with transition width 0.4 K. We also found that the samples possess very large current carrying ability and high upper critical fields, indicating potential applications requiring very high field. The above simple and safe one-step technique of single crystal growth can be effective in other systems of Fe-based superconductors.

preprint2009arXiv

Fabrication and characterization of iron pnictide wires and bulk materials through the powder-in-tube method

The recent discovery of superconductivity in the iron based superconductors with very high upper critical fields presents a new possibility for practical applications, but fabricating fine-wire is a challenge because of mechanically hard and brittle powders and the toxicity and volatility of arsenic. In this paper, we report the synthesis and the physical characterization of iron pnictide wires and bulks prepared by the powder-in-tube method (PIT). A new class of high-Tc iron pnictide composite wires, such as LaFeAsO1-xFx, SmFeAsO1-xFx and Sr1-xKxFeAs, has been fabricated by the in situ PIT technique using Fe, Ta and Nb tubes. Microscopy and x-ray analysis show that the superconducting core is continuous, and retains phase composition after wire drawing and heat treatment. Furthermore, the wires exhibit a very weak Jc-field dependence behavior even at high temperatures. The upper critical field Hc2(0) value can exceed 100 T, surpassing those of MgB2 and all the low temperature superconductors and indicating a strong potential for applications requiring very high field. These results demonstrate the feasibility of producing superconducting pnictide composite wire. We also applied the one step PIT method to synthesize the iron-based bulks, due to its convenience and safety. In fact, by using this technique, we have successfully discovered superconductivity at 35 K and 15 K in Eu0.7Na0.3Fe2As2 and SmCoFeAsO compounds, respectively. These clearly suggest that the one-step PIT technique is unique and versatile and hence can be tailored easily for other rare earth derivatives of novel iron-based superconductors.

preprint2009arXiv

Large transport critical currents of powder-in-tube Sr0.6K0.4Fe2As2/Ag superconducting wires and tapes

We report significant transport critical currents firstly achieved in Sr0.6K0.4Fe2As2 wires and tapes with a Tc = 34 K, which were fabricated through an in-situ powder-in-tube process. Silver was used as a chemical addition as well as a sheath material. Transport measurements were performed by a standard four-probe resistive method. All the wire and tape samples have shown transport properties. Critical current density Jc was enhanced upon silver addition, and at 4.2 K, a best Jc of ~1200 A/cm^2 (Ic = 9 A) was achieved for 20 % silver added tapes, which is the highest in iron-based wires and tapes so far. The Jc is almost field independent between 1 T and 10 T, exhibiting a strong vortex pinning. Such a high transport critical current density is attributed to the absence of reaction layer between the silver sheath and superconducting core, as well as an improved connectivity between grains. We also identify a weak-link behavior from the creep drop of Jc at low fields and a hysteretic phenomenon. Finally, we found that compared to Fe, Ta and Nb tubes, Ag was the best sheath material for the fabrication of high-performance 122 type pnictide wires and tapes.

preprint2009arXiv

Superconductivity in SmFe1-xMxAsO (M = Co, Rh, Ir)

In this paper we report the comparative study of superconductivity by 3d (Co), 4d (Rh), 5d (Ir) element doping in SmFeAsO. X-ray diffraction patterns indicate that the material has formed the ZrCuSiAs-type structure with a space group P4/nmm. It is found that the antiferromagnetic spin-density-wave (SDW) order in the parent compounds is rapidly suppressed by Co, Rh, and Ir doping, and superconductivity emerges. Both electrical resistance and magnetization measurements show superconductivity up to around 10 K in SmFe1-xMxAsO (M = Co, Rh, Ir). Co, Rh and Ir locate in the same column in the periodic table of elements but have different electronic band structure, so comparative study would add more ingredients to the underlying physics of the iron-based superconductors.

preprint2009arXiv

Superconductivity induced by doping Ru in SrFe2-xRuxAs2

Using one-step solid state reaction method, we have successfully synthesized the superconductor SrFe1-xRuxAs. X-ray diffraction indicates that the material has formed the ThCr2Si2-type structure with a space group I4/mmm. The systematic evolution of the lattice constants demonstrates that the Fe ions are successfully replaced by the Ru. By increasing the doping content of Ru, the spin-density-wave (SDW) transition in the parent compound is suppressed and superconductivity emerges. The maximum superconducting transition temperature is found at 13.5 K with the doping level of x = 0.7. The temperature dependence of DC magnetization confirms superconducting transitions at around 12 K. Our results indicate that similar to non-isoelectronic substitution, isoelectronic substitution contributes to changes in both the carrier concentration and internal pressure, and superconductivity could be induced by isoelectronic substitution.

preprint2009arXiv

Superconductivity of powder-in-tube Sr0.6K0.4Fe2As2 wires

Nb-sheathed Sr0.6K0.4Fe2As2 superconducting wires have been fabricated using the powder-in-tube (PIT) method for the first time and the superconducting properties of the wires have been investigated. The transition temperature (Tc) of the Sr0.6K0.4Fe2As2 wires is confirmed to be as high as 35.3 K. Most importantly, Sr0.6K0.4Fe2As2 wires exhibit a very weak Jc-field dependence behavior even the temperature is very close to Tc. The upper critical field Hc2(0) value can exceed 140 T, surpassing those of MgB2 and all the low temperature superconductors. Such high Hc2 and superior Jc-field performance make the 122 phase SrKFeAs wire conductors a powerful competitor potentially useful in very high field applications.

preprint2009arXiv

The role of silver addition on the structural and superconducting properties of polycrystalline Sr0.6K0.4Fe2As2

The effect of Ag addition (0-20 wt%) on polycrystalline Sr0.6K0.4Fe2As2 superconductor has been investigated. It is found that the critical transition temperature Tc was not depressed, and the irreversibility field Hirr and hysteresis magnetization were significantly enhanced upon Ag addition. Characterization study reveals that larger grains are observed in the Ag-added samples. Moreover, the formation of glassy phase as well as amorphous layer, which are present in almost all the grain edges and boundaries in pure samples, are suppressed by Ag addition. The improvement of superconducting properties in Ag-added samples may originate from the enlargement of grains as well as better connections between grains