Structural properties and phase diagram of the $La(Fe_{1-x}Ru_x)AsO$ system
Structural refinement, lattice microstrain and spontaneous strain analyses have been carried out and a phase diagram has been drawn.
Discover
Research tools
Network
Opportunities
Account
Source author record
C. Curfs appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.
Catalog footprint
Research graph
Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.
BZPEER is loading the nearby papers, people, topics and institutions for this page.
Published work
Structural refinement, lattice microstrain and spontaneous strain analyses have been carried out and a phase diagram has been drawn.
Specific heat, resistivity, magnetic susceptibility, linear thermal expansion (LTE), and high-resolution synchrotron X-ray powder diffraction investigations of single crystals Fe1+yTe (0.06 < y < 0.15) reveal a splitting of a single, first-order transition for y < 0.11 into two transitions for y > 0.12. Most strikingly, all measurements on identical samples Fe1.13Te consistently indicate that, upon cooling, the magnetic transition at T_N precedes the first-order structural transition at a lower temperature T_s. The structural transition in turn coincides with a change in the character of the magnetic structure. The LTE measurements along the crystallographic c-axis displays a small distortion close to T_N due to a lattice striction as a consequence of magnetic ordering, and a much larger change at T_s. The lattice symmetry changes, however, only below T_s as indicated by powder X-ray diffraction. This behavior is in stark contrast to the sequence in which the phase transitions occur in Fe pnictides.
A combination of synchrotron X-ray, neutron powder diffraction, magnetization, heat capacity and electrical resistivity measurements reveals that NdMnAsO is an antiferromagnetic semiconductor with large Neel temperature (TN = 359(2) K). At room temperature the magnetic propagation vector k = 0 and the Mn moments are directed along the crystallographic c-axis (mMn = 2.41(6) BM). Upon cooling a spin reorientation (SR) transition of the Mn moments into the ab-plane occurs (TSR = 23 K). This coincides with the long range ordering of the Nd moments, which are restricted to the basal plane. The magnetic propagation vector remains k = 0. At base temperature (1.6 K) the fitted moments are mab,Mn = 3.72(1) BM and mab,Nd = 1.94(1) BM. The electrical resistivity is characterized by a broad maximum at 250 K, below which it has a metallic temperature dependence but semiconducting magnitude (rho250K = 50 Ohm cm, residual resistivity ratio = 2), and a slight upturn at the SR transition.