Source author record

Bunshi Fugetsu

Bunshi Fugetsu appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.

ResearcherUnclaimed source record

Catalog footprint

What is connected

2works
1topics
1close collaborators

Actions

Connect this record

Log in to claim

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

2 published item(s)

preprint2013arXiv

Effect of encapsulated graphene oxide on alginate-based bead adsorption to remove acridine orange from aqueous solutions

Environmentally-benign high-performance graphene oxide (GO)/alginate-based absorbents were prepared to eliminate acridine orange selected as a typical dye. Characterizations demonstrated GO well encapsulated and its promotion of pore formation on structure. Kinetic studies exhibited that the addition of GO shortened the adsorption equilibrium time, raised the initial rate and the adsorption capacity. Isotherm studies indicated the adsorptive behavior followed Langmuir type, and higher maximum capacity was obtained in the presence of GO. The adsorption positively responded to pH increased from acidic to weakly alkaline. At low pH, GO would contribute dominantly to the adsorption, whereas alginate component was inhibited.

preprint2013arXiv

Massive production of graphene oxide from expanded graphite

In a deviation from the conventional Hummers method, a spontaneous expansion approach was introduced with expanded graphite as the precursors. The intercalating agent (H2SO4) was able to penetrate into the expanded graphite; this had further expanded the graphite and as a result, a foam-like intermediate was produced. The foam-like graphite was more easily oxidized in reaction with the oxidant (KMnO4) to form graphene oxide (GO). Fully exfoliated GO was obtained with expanded graphite having the median diameter ~ 15 μm as the precursors. This procedure was much safer and productive in scalable applications than the conventional Hummers methods.