Influence of hydrogenation on the vibrational density of states of magnetocaloric $\mathrm{LaFe}_\mathrm{11.4}\mathrm{Si}_\mathrm{1.6}\mathrm{H}_{1.6}$
We report on the impact of magnetoelastic coupling on the magnetocaloric properties of LaFe$_{11.4}$Si$_{1.6}$H$_{1.6}$ in terms of the vibrational density of states, which we determined with $^{57}$Fe nuclear resonant inelastic X-ray scattering measurements and with density-functional-theory based first-principles calculations in the ferromagnetic low-temperature and paramagnetic high-temperature phase. In experiments and calculations, we observe pronounced differences in the shape of the Fe-partial VDOS between non-hydrogenated and hydrogenated samples. This shows that hydrogen does not only shift the temperature of the first-order phase transition, but also affects the elastic response of the Fe-subsystem significantly. In turn, the anomalous redshift of the Fe VDOS, observed by going to the low-volume PM phase, survives hydrogenation. As a consequence, the change in the Fe specific vibrational entropy $ΔS_\mathrm{lat}$ across the phase transition has the same sign as the magnetic and electronic contribution. DFT calculations show that the same mechanism, which is a consequence of the itinerant electron metamagnetism associated with the Fe subsystem, is effective in both the hydrogenated and he hydrogen-free compounds. Although reduced by 50 % as compared to the hydrogen-free system, the measured change $ΔS_\mathrm{lat}$ of 3.2\pm1.9 J/kgK across the FM to PM transition contributes with 35 % significantly and cooperatively to the total isothermal entropy change $ΔS_\mathrm{iso}$. Hydrogenation is observed to induce an overall blueshift of the Fe-VDOS with respect to the H-free compound; this effect, together with the enhanced Debye temperature observed, is a fingerprint of the hardening of the Fe sublattice by hydrogen incorporation. In addition, the mean Debye velocity of sound of LaFe$_{11.4}$Si$_{1.6}$H$_{1.6}$ was determined from the NRIXS and the DFT data.