Source author record

A. J. Craven

A. J. Craven appears in the imported research catalog. Authorship, coauthor and topic links are available while profile ownership is still unclaimed.

ResearcherUnclaimed source record

Catalog footprint

What is connected

2works
2topics
4close collaborators

Actions

Connect this record

Log in to claim

Research graph

See the researcher in context

Open full explorer

Inspect adjacent papers, topics, institutions and collaborators without losing the researcher page.

Building this map preview

BZPEER is loading the nearby papers, people, topics and institutions for this page.

Published work

2 published item(s)

preprint2014arXiv

Enhanced Eshelby Twist on Thin Wurtzite InP Nanowires and Measurement of Local Crystal Rotation

We have performed a detailed study of the lattice distortions of InP wurtzite nanowires containing an axial screw dislocation. Eshelby predicted that this kind of system should show a crystal rotation due to the dislocation induced torque. We have measured the twisting rate and the dislocation Burgers vector on individual wires, revealing that nanowires with a 10-nm radius have a twist up to 100% larger than estimated from elasticity theory. The strain induced by the deformation has a Mexican-hat-like geometry, which may create a tube-like potential well for carriers.

preprint2013arXiv

Characterization of Fe-N nano crystals and nitrogen-containing inclusions in (Ga,Fe)N thin films using transmission electron microscopy

Nanometric inclusions filled with nitrogen, located adjacent to FenN (n = 3 or 4) nanocrystals within (Ga,Fe)N layers, are identified and characterized using scanning transmission electron microscopy (STEM) and electron energy-loss spectroscopy (EELS). High-resolution STEM images reveal a truncation of the Fe-N nanocrystals at their boundaries with the nitrogen-containing inclusion. A controlled electron beam hole drilling experiment is used to release nitrogen gas from an inclusion in situ in the electron microscope. The density of nitrogen in an individual inclusion is measured to be 1.4 +- 0.3 g/cm3. These observations provide an explanation for the location of surplus nitrogen in the (Ga,Fe)N layers, which is liberated by the nucleation of FenN (n> 1) nanocrystals during growth.